Stainless Steel 317 / 317L Pipe Fittings
ASME SA403 SS 317 Long Stub, SS 317L Pipe bend, SS 317L Short Radius Elbow, SS WP317 Pipe Elbow, ANSI B16.9 Stainless Steel 317L Welded Buttweld Fittings, SS WERKSTOFF NR.1.4449 Cross Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading manufacturing and supplying firm of Stainless Steel 317 / 317L Butt Weld Pipe Fittings, which is non-magnetic in the annealed condition. Stainless Steel 317 Elbow Pipe Fittingsis molybdenum containing austenitic alloy. Stainless Steel 317L Tee Pipe Fittings has good formability and weldability. Stainless Steel 317 Cross Pipe Fittings is used in chemical and petrochemical process equipment. Stainless Steel 317L Reducer Pipe Fittings combines good corrosion resistance with good mechanical properties and fabricability. Stainless Steel 317 Bend Pipe Fittings is often used in screens for marine and chemical applications. Stainless Steel 317L Stub End Pipe Fittings provides resistance to sensitization during welding and other thermal processes.
Stainless Steel 317 End Cap Pipe Fittings is tougher steel with a long stringy chip; however, using chip breakers is recommended. Stainless Steel 317L Dish Cap Pipe Fittings has improved resistance to chlorides and other corrosives. Stainless Steel 317 Lateral Tee Pipe Fittings offers stress-to-rupture, higher creep, and tensile strength at elevated temperature. Low speeds and constant feeds will minimize the tendency of Stainless Steel UNS S31700 Pipe Fittings to work harden. Due to its low carbon content, Stainless Steel UNS S31703 Pipe Fittings also provides resistance to sensitization when welded. 317 Stainless Steel Pipe Fittings has the highest tensileand creep strength properties at elevated temperatures. 317L Stainless Steel Pipe Fittings are used in the Food, Marine, Pharmaceutical, and Architecture industries.
317L Stainless Steel End Cap, 317L Stainless Steel Reducer, 317 SS Short Radius Elbow, SS 1.5d Pipe Bend, SS 317 End Pipe Cap, 317L Stainless Steel Reducer, SS 317L Pipe Reducer, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 317 / 317L Pipe Fittings Specifications
| Grade | SS 317 | UNS S31700 |
| Standard | ASTM A403 / ASME SA403 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| STANDARD | SS 317 |
| UNS | S31700 |
| WERKSTOFF NR. | 1.4449 |
| AFNOR | - |
| JIS | SUS 317 |
| GOST | - |
| BS | - |
| EN | - |
Stainless Steel 317 / 317L Pipe Fittings Chemical Composition
| Grade | C | Ni | Mn | P | S | Cr | Si | Mo | Fe |
| 317 | 0.08 max | 11.00 – 15.00 | 2 max | 0.045 max | 0.030 max | 18.00 – 20.00 | 1 max | 3.00 – 4.00 | 57.845 min |
| SS 317L | 0.035 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 18.00 – 20.00 | 3.00 – 4.00 | 11.00 – 15.00 | 57.89 min |
Stainless Steel 317 / 317L Pipe Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.9 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
Other Types of Stainless Steel 317 / 317L Pipe Fittings
- SS 317/317L Buttweld Tee Supplier in UAE
- Stainless UNS S31700 Cross Manufacturer in India
- SS 317/317L Butwteld Tee
- DIN 1.4449 45deg.Elbow
- DIN 1.4449 Buttweld Pipe Fittings
- 317 Steel Short Radius Elbow
- UNS S31700 Ecentric Reducer Distributors
- SS 317L Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 317 Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 317 U Bend
- WNR. 1.4449 SS 317L Stub End Supplier in Poland
- 317 Short Radius Elbow
- WP 317L Steel Equal Tee in Qatar
- UNS S31700 End Cap
- ASME SA403 Concentric Reducer
- SS 317L Seamless Fitting
- Stainless Steel 317 45 Elbow
- SS 317L Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 317 / 317L Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 317 / 317L Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo