Super Duplex Steel UNS S32750 / S32760 Pipe Fittings
Super Duplex S32760 Pipe Fittings, S32750 Super Duplex End Cap, Super Duplex SAF 2507 Pipe Elbow, Super Duplex WERKSTOFF NR. 1.4410 Cross, UNS S32750 Short & Long Radius Elbow, UNS S32760 Equal Tee & Unequal Tee Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the notable exporters of Super Duplex Steel S32750 / S32760 Butt Weld Pipe Fittings, which is used in oil and gas industry equipment. Super Duplex S32750 Elbow Pipe Fittings is particularly suited for use in aggressive environments. Super Duplex S32760 Tee Pipe Fittingshas high yield strength and tensile strength. Super Duplex S32750 Reducer Pipe Fittings exhibits high thermal conductivity and low thermal expansion. Super Duplex S32760 Cross Pipe Fittings is supplied with a PREN (Pitting Resistance Equivalent) which guarantees high resistance to pitting corrosion.In dilute sulfuric acid contaminated with chloride ions, Super Duplex S32750 CapPipe Fittingshas better corrosion resistance.
Super Duplex S32760 Bend Pipe Fittingsis designed to feature erosion corrosion and corrosion fatigue, crevice corrosion and strong weldability. Super Duplex S32750 Stub End Pipe Fittingshas improved strength over ferritic and austenitic steel grades. High molybdenum, chromium and nitrogen content in Super Duplex S32760 End CapPipe Fittings help the material withstand pitting and crevice corrosion. Super Duplex S32750 Dish Cap Pipe Fittings results in excellent resistance to chloride pitting and crevice corrosion attack. Super Duplex S32760 Lateral TeePipe Fittingsprovides pitting and crevice corrosion resistance superior to austenitic and duplex stainless steels in almost all corrosive media, and a Critical Pitting Temperature exceeding 50 Degree C. Super Duplex 2507 Pipe Fittings has good weldability and can be welded by several methods.
Super Duplex S32750/ S32760 180 Degree Elbow, Super Duplex S32760 Long & Short Stub End, ASTM A/ASME SA815 Super Duplex S32750 Lateral Tee, Duplex 3D Bend, S32760 Super Duplex Steel Reducer Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Super Duplex UNS S32750 / S32760 Pipe Fittings Specifications
| Grade | UNS S32750/S32760, Super Duplex Steel |
| Standard | ASTM B815 / ASME SB815 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 24" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| Standard | Super Duplex Steel S2507 |
| Werkstoff Nr. | 1.4410 |
| UNS | S32750 | S32760 |
| JIS | - |
| AFNOR | - |
| BS | - |
| GOST | - |
| EN | - |
Super Duplex UNS S32750 / S32760 Pipe Fittings Chemical Composition
| Grade | C | Si | Mn | P | S | Cr | Mo | Ni | N | Other |
| 2507 | 0.030 | 0.80 | 1.20 | 0.035 | 0.020 | 24.0/26.0 | 3.0/5.0 | 6.00/8.00 | 0.24/0.32 | Cu:0.50 |
Super Duplex UNS S32750 / S32760 Pipe Fittings Mechanical Properties
| Grade | Proof Stress 0.2% (MPa) |
Tensile Strength (MPa) |
Elongation A5(%) |
Hardness Max | |
| HB | HRB | ||||
| 2507 | 550 | 795 | 15 | 310 | 32* |
Other Types of Super Duplex UNS S32750 / S32760 Pipe Fittings
- UNS S31803 Buttweld Tee Supplier in UAE
- UNS S32205 Cross Manufacturer in India
- DIN 1.4462 Butwteld Tee
- DIN 1.4462 45 deg.Elbow
- UNS S31803 Buttweld Pipe Fittings
- UNS S32205 Short Radius Elbow
- UNS S31803 Ecentric Reducer Distributors
- UNS S32205 Buttweld Pipe Fitting
- ASME SB337 Stub End
- Duplex Steel Concentric Reducer
- UNS S31803 Long Radius Elbow Exporter in Russia
- UNS S32005 U Bend
- Duplex Steel Stub End Supplier in Poland
- Duplex Steel Short Radius Elbow
- UNS S31803 Equal Tee in Qatar
- UNS S32205 End Cap
- ASTM B337 Concentric Reducer
- Duplex Steel Seamless Fitting
- UNS S31803 180 Deg Elbow
- UNS S32205 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Duplex UNS S31803 / S32205 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Duplex UNS S31803 / S32205 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo