Copper Nickel 90/10 Pipe Fittings
90/10 Cupro Nickel Long & Short Radius Elbow, Cu-Ni 90/10 Pipe Elbow, Copper Nickel 90/10 180 Degree Elbow, Cupro Nickel 3D Pipe Bend, ASME SB366 Cupro Nickel 90-10 Long Stub End Manufacturer in Mumbai,India.
Nickel Super Alloys is a renowned distributor of Copper Nickel 90/10 Butt Weld Pipe Fittings, which resists corrosion by fast moving water.Combined with high ductility and toughness, Cupro Nickel 90 / 10 Elbow Pipe Fittings makes a popular grade for marine, architectural and industrial applications. Cu-Ni 90 / 10 Tee Pipe Fittings is chosen for sea water service that contains 10 percent or 30 percent of nickel content.The high oxidation resistance of these Copper Nickel / 10 Cross Pipe Fittings is visible in moist air and steam. Cupro Nickel 90 / 10 Reducer Pipe Fittings with additions of manganese are important in electrical engineering. Cu-Ni 90 / 10 Cap Pipe Fittings is highly resistant to corrosion by salt water, and is therefore used for piping.
Copper Nickel 90 / 10 Bend Pipe Fittings failures due to stress-corrosion cracking are unknown in seawater polluted with ammonia. Cupro Nickel 90 / 10 Stub End Pipe Fittings provides an assessment of the corrosion resisting characteristics. Cu-Ni 90 / 10 End Cap Pipe Fittings have good strength at moderately elevated temperatures. The inclusion of controlled quantities of iron and manganese also give Copper Nickel 90 / 10 Dish Cap Pipe Fittingsan extraordinary resistance to general corrosion and stress cracking. Copper Nickel C70600 Pipe Fittings can be found in seawater systems for naval, commercial shipping and the oil & gas markets due to its good strength.
ASTM B366 Cupro Nickel 90/10 90 Dgree Elbow, Copper Nickel WERKSTOFF NR. 2.0872 Cross, 90/10 Cupro Nickel 180 Deg bend, 90/10 Cu-Ni Pipe Reducer, Cu-Ni UNS C70600 Seamless Pipe Fittings Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Cupro Nickel 90/10 Pipe Fittings Specifications
| Grade | Copper Nickel 90-10 / UNS C70600 Werkstoff Nr. 2.0872 |
| Standard | ASTM B122, B171, B466, B467 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Size | 1/2" to 24" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
Cupro Nickel 90/10 Pipe Fittings Chemical Composition
| Cu-Ni 90/10 | Cu | Pb | Mn | Fe | Zn | Ni |
| 88.6 min | 0.05 max | 1.0 max | 1.8 max | 1 max | 9-11 max |
Cupro Nickel 90/10 Pipe Fittings Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.1 g/cm3 | 1443 °C (2430 °F) | Psi – 35,000, MPa – 241 | Psi -80,000, MPa -551 | 30 % |
Other Types of Cupro Nickel 90/10 Pipe Fittings
- Cu-Ni 90-10 Buttweld Tee Supplier in UAE
- UNS C70600 Cross Manufacturer in India
- DIN 2.0872 Butwteld Tee
- DIN 2.0872 45 deg.Elbow
- Cu-Ni 90-10 Buttweld Pipe Fittings
- Copper Nickel 90-10 Short Radius Elbow
- Cupro Nickel 90-10 Ecentric Reducer Distributors
- UNS C70600 Buttweld Pipe Fitting
- ASME B16.9 Stub End
- Cupro Nickel 90-10 Concentric Reducer
- Cupro Nickel 90-10 Long Radius Elbow Exporter in Russia
- Copper Nickel 90-10 U Bend
- Cupro Nickel 90-10 Stub End Supplier in Poland
- Cu-Ni 90-10 Short Radius Elbow
- UNS C70600 Equal Tee in Qatar
- Cu-Ni 90-10 End Cap
- ASTM B122 Concentric Reducer
- Cu-Ni 90-10 Seamless Fitting
- Cu-Ni 90-10 180 Deg Elbow
- Cu-Ni 90-10 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Copper Nickel 90-10 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Copper Nickel 90-10 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo