Stainless Steel 304 / 304L Pipe Fittings
ASTM A403 WP 304 Stainless Steel 90 degree Elbow, Stainless Steel 304L Pipe Elbow, SS 304 Short Radius Elbow, Stainless Steel 304L Pipe Fittings,SS WERKSTOFF NR. 1.4301 Cross, UNS S30400 Short Stub end Manufacturer in Mumbai,India.
Nickel Super Alloys is one of leading supplier and distributor of Stainless Steel 304 / 304L Butt Weld Pipe Fittings, which is the most widely used austenitic (non-magnetic) stainless steel. Stainless Steel 304 Elbow Pipe Fittings is the standard “18/8 stainless” that is commonly found in pans and cooking tools. Stainless Steel 304L Tee Pipe Fittings can be used in an "as welded" condition. Essentially, Stainless Steel 304 Lateral Tee Pipe Fittings is an austenitic chromium alloy which is also known as an "18/8" stainless as the make-up of the steel is 18 percent chromium and 8 percent nickel. Stainless Steel 304L Cross Pipe Fittings has high ductility, excellent forming, spinning and drawing properties.
This property has resulted in Stainless Steel 304 Reducer Pipe Fittings being the dominant grade used in applications like sinks and saucepans. Stainless Steel 304L Bend Pipe Fittings depends on the temperature and subsequently exposed to aggressive corrosive environments. Stainless Steel 304 Stub End Pipe Fittings is combined with an addition of nitrogen that enables to meet the excellent mechanical properties. Stainless Steel 304L End Cap Pipe Fittings is welded or otherwise heated at temperatures between 430 Degree C and 860 Degree C. Stainless Steel 304 Dish Cap Pipe Fittings exhibit good machinability. Stainless Steel UNS S30400 Pipe Fittings creates other entries for more specific heat treatments and forms. Stainless Steel UNS S30403 Pipe Fittings has lower carbon content to minimize carbide precipitation.
Stainless Steel UNS S30403 Seamless Pipe Fittings, Stainless Steel 304 U bend, SS 3D Pipe Bend, SS WP 304L 45 degree Elbow, Stainless Steel UNS S30400 Seamless 3D Pipe Bend Fittings, WNR. 1.4301 SS 304 Stub End Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 304 / 304L Pipe Fittings Specifications
| Grade | SS 304 | Stainless Steel 304 | UNS S30400 |
| Standard | ASTM A403 / ASME SA403 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| STANDARD | UNS | AFNOR | JIS | WERKSTOFF NR. | EN | BS | GOST |
| SS 304 | S30400 | Z7CN18‐09 | SUS 304 | 1.4301 | X5CrNi18-10 | 304S31 | 08Х18Н10 |
Stainless Steel 304 / 304L Pipe Fittings Chemical Composition
| Element | Ni | C | Mn | P | S | Si | Cr |
| SS 304 | 8.0 – 11.0 | 0.08 | 2.0 max | 0.045 max | 0.03 max | 1.0 max | 18.0 – 20.0 |
| SS 304L | 8.0 – 13.0 | 0.35 | 2.0 max | 0.045 max | 0.03 max | 1.0 max | 18.0 – 20.0 |
Stainless Steel 304 / 304L Pipe Fittings Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 304/304L | 515 | 205 | 40 | 92 | 201 |
Other Types of Stainless Steel 304 / 304L Pipe Fittings
- SS 304/304L Buttweld Tee Supplier in UAE
- Stainless UNS S30400 Cross Manufacturer in India
- SS 304/304L Butwteld Tee
- DIN 1.4307 45deg.Elbow
- DIN 1.4306 Buttweld Pipe Fittings
- 304 Steel Short Radius Elbow
- UNS S30400 Ecentric Reducer Distributors
- SS 304 Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 304 Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 304 U Bend
- WNR. 1.4301 SS 304 Stub End Supplier in Poland
- 304 Short Radius Elbow
- WP 304 Steel Equal Tee in Qatar
- UNS S30400 End Cap
- ASME SA403 Concentric Reducer
- SS 304 Seamless Fitting
- Stainless Steel 304 45 Elbow
- SS 304 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 304 / 304L Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 304 / 304L Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo