Stainless Steel 310 / 310S Pipe Fittings
SS UNS S31008 Welded Pipe Fittings, SS 310 Buttweld Pipe Fittings, UNS S31000 Steel Elbow, SS 310 Steel Tee, 310 Steel Reducers, SS 310S Long Stub bends Manufacturer in Mumbai,India.
Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310 / 310S Butt Weld Pipe Fittings, which is the choice for high temperature applications. Stainless Steel 310 Pipe Fittings has good resistance in intermittent service and 1150 Degree C (2102 Degree F) in continuous service. Preheating is not necessary for Stainless Steel 310S Elbow Pipe Fittings, and so it is suitable for use in high temperatures. Stainless Steel 310 Tee Pipe Fittings has higher carbon content that minimizes carbide precipitation and improves weldability. The key properties of Stainless Steel 310S Cross Pipe Fittings are its high chromium and medium nickel content.
As a result of its high chromium and nickel content, Stainless Steel 310 Reducer Pipe Fittings has good resistance to sulphidation and other forms of hot corrosion. Stainless Steel 310S Bend Pipe Fittings has superior resistance to oxidation, which forms a tenacious scale at high temperature. Because of its high chromium and moderate nickel content, Stainless Steel 310 Stub End Pipe Fittings and can also be used in moderately carburizing atmospheres. Stainless Steel 310S End Cap Pipe Fittings is used in fluidised bed combustors, kilns and radiant tubes. As it has excellent resistance to oxidation, therefore Stainless Steel UNS S31000 Pipe Fittings has superior strength in temperatures up to 2100 Degree F. Stainless Steel UNS S31008 Pipe Fittings is a highly alloyed austenitic stainless steel used for high temperature application.
Stainless Steel 310 Short Radius Elbow, UNS S31000 90 Degree Elbow, SS 310S Pipe Cross, SS 310/310S Bends, SS WERKSTOFF NR. 1.4841 Eccentric Reducer, UNS S31008 End & Dish Cap Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 310 / 310S Pipe Fittings Specifications
| Grade | SS 310/310S | Stainless Steel 310/310S |
| Standard | ASTM A403 / ASME SA403 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| STANDARD | SS 310 | SS 310S |
| UNS | S31000 | S31008 |
| WERKSTOFF NR. | 1.4841 | 1.4845 |
| JIS | SUS 310 | SUS 310S |
| BS | 310S24 | 310S16 |
| GOST | 20Ch25N20S2 | 20Ch23N18 |
| AFNOR | - | - |
| EN | X15CrNi25-20 | X8CrNi25-21 |
Stainless Steel 310 / 310S Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SS 310 | 0.015 max | 2 max | 0.015 max | 0.020 max | 0.015 max | 24.00 – 26.00 | 0.10 max | 19.00 – 21.00 | 54.7 min |
| SS 310S | 0.08 max | 2 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | 0.75 max | 19.00 – 21.00 | 53.095 min |
Stainless Steel 310 / 310S Pipe Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |
Other Types of Stainless Steel 310 / 310S Pipe Fittings
- SS 310 Buttweld Tee Supplier in UAE
- Stainless UNS S31000 / S31008 Cross Manufacturer in India
- SS 310s Butwteld Tee
- DIN 1.4841 45deg.Elbow
- DIN 1.4845 Buttweld Pipe Fittings
- 310 Steel Short Radius Elbow
- UNS S31000 Ecentric Reducer Distributors
- SS 310S Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 310 Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 310s U Bend
- WNR. 1.4841 SS 310 Stub End Supplier in Poland
- 310S Short Radius Elbow
- WP 310 Steel Equal Tee in Qatar
- UNS S31000 End Cap
- ASME SA403 Concentric Reducer
- SS 310S Seamless Fitting
- Stainless Steel 310 45 Elbow
- SS 310S Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo