Inconel 600 Pipe Fittings
ANSI B16.9 Inconel 600 Welded Pipe Fittings, Inconel 600 Pipe Elbow, Inconel WERKSTOFF NR. 2.4816 Cross, 600 Inconel Alloy End Cap, ASTM B366 600 Inconel Alloy 90 degree Elbow Manufacturer in Mumbai, India.
Nickel Super Alloys Steel is one of the prominent manufacturers, suppliers and exporters of Inconel Alloy 600 Butt Weld Pipe Fittings, which has excellent mechanical properties. Inconel 600 Elbow Pipe Fittings is combination of Nickel Chromium and Iron provides a standard material for the chemical industry and the automotive engine, airframe and aero-engine sectors. When heated, Inconel 600 Tee Pipe Fittings forms a stable, thick, passivation oxide layer protecting the surface from further attack. Apart from good carburization resistance, Inconel 600 Reducer Pipe Fittingshas an excellent oxidation resistance up to 1093 Degree C. Inconel 600 Cross Pipe Fittings has good SCC resistance property in both room temperature and high temperature.
Inconel 600 Bend Pipe Fittings is used for chemical processing, furnace components, and food processing. Inconel 600 Stub End Pipe Fittings is designed for use at cryogenic temperatures and up to 2000 Degree F. Inconel 600 End Cap Pipe Fittings is non-magnetic and readily weldable. Inconel 600 Dish Cap Pipe Fittings has long been used in the heat treating industry. Inconel 600 Lateral Tee Pipe Fittings has great resistance to heat and corrosion. Application of Inconel 600 Concentric Reducer Pipe Fittingsis useful in the chemical, pulp and paper. Inconel 600 Eccentric Reducer Pipe Fittings presents the desirable combination of good weldabilityand high strength under a wide range of temperatures. The high nickel contentgives Inconel UNS N06600 Pipe Fittings resistance to corrosion by many organic and inorganic compounds.
Inconel 600 Pipe Fittings, ASME SB366 Inconel 600 Long Stub, 600 Inconel Eccentric & Concentric Reducer, ASME SB366 Inconel 600 Long Stub, Alloy 600 Short Radius Elbow, Inconel UNS N06600 Seamless Pipe Fittings Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Inconel 600 Pipe Fittings Specifications
| Grade | Inconel Alloy 600 / UNS N06600 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Inconel 600 Seamless Fittings | 1/2" NB - 10" NB |
| Inconel 600 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Inconel 600 |
| UNS | N06600 |
| GOST | МНЖМц 28-2,5-1,5 |
| BS | NA 13 |
| JIS | NCF 600 |
| AFNOR | NC15FE11M |
| WERKSTOFF NR. | 2.4816 |
| EN | NiCr15Fe |
| OR | ЭИ868 |
Inconel 600 Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
Inconel 600 Pipe Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
Other Types of Inconel 600 Pipe Fittings
- Inconel 600 Buttweld Tee Supplier in UAE
- UNS N06600 Cross Manufacturer in India
- Inconel 600 Butwteld Tee
- DIN 2.4816 45 deg.Elbow
- DIN 2.4816 Buttweld Pipe Fittings
- Inconel 600 Short Radius Elbow
- UNS N06600 Ecentric Reducer Distributors
- Inconel 600 Buttweld Pipe Fitting
- ASME SB366 Stub End
- 600 Inconel Concentric Reducer
- ASTM B366 Inconel 600 Long Radius Elbow Exporter in Russia
- Inconel 600 U Bend
- Inconel 600 Stub End Supplier in Poland
- 600 Inconel Short Radius Elbow
- Inconel 600 Equal Tee in Qatar
- UNS N06600 End Cap
- ASME SB366 Concentric Reducer
- Inconel 600 Seamless Fitting
- Inconel 600 45 Deg Elbow
- Inconel 600 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Inconel 600 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Inconel 600 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo