Duplex Steel UNS S31803 / S32205 Pipe Fittings
Duplex Steel WERKSTOFF NR. 1.4462 Cross, Duplex Equal Tee, UNS S31803 Duplex Steel Reducer, UNS S32205 180 Degree Elbow, Duplex 1.5d Bend, ASTM A815 UNS S32205 Duplex Steel 90 Degree Elbow Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the prominent suppliers of Duplex Steel S31803 / S32205 Butt Weld Pipe Fittings, which is suitable for applications which involve high mechanical stresses. Duplex Steel S31803 Elbow Pipe Fittings has better localized corrosion resistance than Stainless Steel 316L Pipes and Tubes and Stainless Steel 317L Pipes and Tubes. Duplex Steel S32205 Tee Pipe Fittingsis not generally suitable for use at temperatures above 300 Degree C. Microstructures of Duplex Steel S31803 Cross Pipe Fittingsconsist of a mixture of austenite and ferrite phases. Duplex Steel S32205 Reducer Pipe Fittings also demonstrates good fatigue strength, as well as outstanding resistance to stress corrosion cracking. By agreement, Duplex Steel S31803 Bend Pipe Fittings can be supplied with a PREN (Pitting Resistance Equivalent).
Duplex Steel S32205 Stub End Pipe Fittings has resistance to stress corrosion cracking of importance in many applications including hot water tanks. The greatest corrosion advantage for Duplex Steel S31803 End Cap Pipe Fittings is their improved resistance to CSCCwhen compared to the austenitic grades. In the annealed condition, Duplex Steel S32205 Dish Cap Pipe Fittingscontains approximately 40 percent to 50 percent of ferrite. Duplex Steel S31803 Lateral Tee Pipe Fittings is capable to resist localized corrosion such as pitting, crevice corrosion and SCC. Duplex Steel S32205 Concentric Reducer Pipe Fittings contains larger amounts of chromium in comparison with other steels and thus have good corrosion resistance.
Duplex Steel UNS S31803 Stub Bend, UNS S32205 Duplex End Cap, Duplex Steel 2205 Long & Short Radius Elbow, Duplex Steel S31803 Pipe Fittings, ANSI B16.9 Duplex Steel S32205 Pipe Bend, UNS S31803 Equal Tee, Unequal Tee Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Duplex UNS S31803 / S32205 Pipe Fittings Specifications
| Grade | UNS S31803/S32205, Duplex Steel |
| Standard | ASTM B337 / ASME SB337 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 24" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| Standard | Duplex Steel |
| Werkstoff Nr. | 1.4462 |
| UNS | S31803 | S32205 |
| JIS | - |
| AFNOR | - |
| BS | - |
| GOST | - |
| EN | - |
Duplex UNS S31803 / S32205 Pipe Fittings Chemical Composition
| Grade | ASTM | C | Mn | P | S | Si | Cr | Ni | N | Mo |
| S32205 | 2205 | 0.03 max | 2 max | 0.03 max | 0.02 max | 1 max | 22-23 | 4.5-6.5 | 0.14-0.2 | 3-3.5 |
| SS31803 | 0.03 max | 2 max | 0.03 max | 0.02 max | 1 max | 21-23 | 4.5-6.5 | 0.08-0.2 | 2.5-3.5 |
Duplex UNS S31803 / S32205 Pipe Fittings Mechanical Properties
| Grade | Tensile Strength min | Yield Strength min | Elongation min | Hardness max |
| S32205 | 95 ksi | 65 ksi | 25% | 31 HRC |
| S31803 | 90 ksi | 65 ksi | 25% | 31 HRC |
Other Types of Duplex UNS S31803 / S32205 Pipe Fittings
- UNS S31803 Buttweld Tee Supplier in UAE
- UNS S32205 Cross Manufacturer in India
- DIN 1.4462 Butwteld Tee
- DIN 1.4462 45 deg.Elbow
- UNS S31803 Buttweld Pipe Fittings
- UNS S32205 Short Radius Elbow
- UNS S31803 Ecentric Reducer Distributors
- UNS S32205 Buttweld Pipe Fitting
- ASME SB337 Stub End
- Duplex Steel Concentric Reducer
- UNS S31803 Long Radius Elbow Exporter in Russia
- UNS S32005 U Bend
- Duplex Steel Stub End Supplier in Poland
- Duplex Steel Short Radius Elbow
- UNS S31803 Equal Tee in Qatar
- UNS S32205 End Cap
- ASTM B337 Concentric Reducer
- Duplex Steel Seamless Fitting
- UNS S31803 180 Deg Elbow
- UNS S32205 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Duplex UNS S31803 / S32205 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Duplex UNS S31803 / S32205 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo