Incoloy 800 / 800H / 800HT Pipe Fittings
Alloy 800 Short Radius Elbow, Incoloy UNS N08800 / N08810 / N08811 Seamless Pipe Fittings, 800HT Incoloy Alloy End Cap, Incoloy WERKSTOFF NR. 1.4876 /1.4958 /1.4859 Cross Manufacturer in Mumbai, India.
Nickel Super Alloys is one of leading distributors and suppliers of Inconel Alloy 800 / 800H / 800HT Butt Weld Pipe Fittings, which has good strength and excellent resistance to oxidation. The combined effects of mechanical and thermal processing of Inconel 800 Elbow Pipe Fittings permit higher design stresses. Inconel 800HTee Pipe Fittings has higher creep and rupture properties for high temperature situations above 1100 Degree F (600 Degree C). In addition to the chemistry restrictions, Inconel 800HT Cross Pipe Fittings receives a high temperature annealing treatment that produces an average grain size. Inconel 800 Reducer Pipe Fittings is used in power generation, reheater and superheater tubing.
The strength of Inconel 800H Bend Pipe Fittings is achieved by controlled levels of aluminum, carbon, and titanium along with a 2100 Degree F minimum annealing to achieve a grain size. Inconel 800HT Stub End Pipe Fittings has excellent tensile strength and resistance to oxidation as well as carburization properties. Inconel 800 End Cap Pipe Fittings is typically used for applications involving long-term exposure to high-temperatures. Inconel 800H Dish Cap Pipe Fittings has further modifications to the combined titanium and aluminum levels to ensure optimum high temperature properties. Inconel 800HT Lateral Tee Pipe Fittings has excellent carburization another types of high-temperature corrosion. Inconel 800 Concentric Reducer Pipe Fittings is particularly useful for high-temperature equipment in the petrochemical industry.
Incoloy 800H Pipe Fittings, 800HT Incoloy Alloy End Cap, 800HT Incoloy Reducer, Incoloy 800 180 Degree Elbow, 800HT Incoloy Alloy End Cap, Incoloy Alloy 800 Equal Tee, Incoloy 800H Pipe Elbow, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 800 / 800H / 800HT Pipe Fittings Specifications
| Grade | Incoloy Alloy 800, 800H, 800HT, UNS N08800, N08810, N08811 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Incoloy 800 Seamless Fittings | 1/2" NB - 10" NB |
| Incoloy 800 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Incoloy 800 | Incoloy 800H | Incoloy 800HT |
| UNS | N08800 | N08810 | N08811 |
| EN | X10NiCrAlTi32-20 | X5NiCrAlTi31-20 | X8NiCrAlTi32-21 |
| AFNOR | Z8NC32-21 | Z8NC33-21 | - |
| JIS | NCF 800 | NCF 800H | NCF 800HT |
| BS | NA 15 | NA 15(H) | NA 15(HT) |
| WERKSTOFF NR. | 1.4876 | 1.4958 / 1.4876 | 1.4859 / 1.4876 |
| GOST | ЭИ670 | ЭИ670 | ЭИ670 |
| OR | XH32T | XH32T | XH32T |
Incoloy 800 / 800H / 800HT Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr | Al | Ti |
| 800 | 0.10 max | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60 | 0.15 – 0.60 |
| 800H | 0.05 – 0.10 | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60 | 0.15 – 0.60 |
| 800HT | 0.06 – 0.10 | 1.50 max | 1.00 max | 0.015 max | 0.75 max | 39.50 min | 30.00 – 35.00 | 19.00 – 23.00 | 0.15 – 0.60ᴬ | 0.15 – 0.60ᴬ |
Incoloy 800 / 800H / 800HT Pipe Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 800 / 800H / 800HT | 7.94 g/cm3 | 1385 °C (2525 °F) | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa – 205 | 30 % |
Other Types of Incoloy 800 / 800H / 800HT Pipe Fittings
- Incoloy 800 Buttweld Tee Supplier in UAE
- UNS N08800 / N08810 / N08811 Cross Manufacturer in India
- Incoloy 800H Butwteld Tee
- DIN 1.4876 /1.4958 /1.4859 45 deg.Elbow
- DIN 1.4876 /1.4958 /1.4859 Buttweld Pipe Fittings
- Inconel 625 Short Radius Elbow
- UNS N08800 / N08810 / N08811 Ecentric Reducer Distributors
- Incoloy 800HT Buttweld Pipe Fitting
- ASME SB366 Stub End
- 800 Incoloy Concentric Reducer
- Incoloy 800H Long Radius Elbow Exporter in Russia
- Incoloy 800HT U Bend
- Incoloy 800 Stub End Supplier in Poland
- 800H Incoloy Short Radius Elbow
- Incoloy 800HT Equal Tee in Qatar
- UNS N08800 / N08810 / N08811 End Cap
- ASME SB366 Concentric Reducer
- Incoloy 800 Seamless Fitting
- Incoloy 800H 180 Deg Elbow
- Incoloy 800HT Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 800 / 800H / 800HT Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 800 / 800H / 800HT Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo