Stainless Steel 310H Pipe Fittings
Stainless Steel 310H Pipe Fittings, SS 310H Buttweld Pipe Fittings, 310H Stainless Steel Seamless Fitting, SS UNS S31009 Welded Pipe Fittings, SS 310H 90 Degree Elbow, UNS S31009 End & Dish Cap, Manufacturer in Mumbai,India.
Nickel Super Alloys is a prominent firm in exporting and manufacturing Stainless Steel 310H Butt Weld Pipe Fittings, which is resistance to hot corrosion. Stainless Steel 310H Elbow Pipe Fittingsis used in Retorts linings, Refractory supports and Conveyor belts. The high chromium content – intended to increase high temperature properties – also gives Stainless Steel 310H Tee Pipe Fittings good aqueous corrosion resistance .Stainless Steel 310H Cross Pipe Fittings has an extensively higher coefficient of thermal expansion as non-alloyed steels. Stainless Steel 310H Reducer Pipe Fittingshas good mechanical strength at elevated temperatures. Stainless Steel 310H Bend Pipe Fittingshas good machinability and is readily fabricated.
When heated in the range of 1202 Degree F – 1742 Degree F (650 Degree C – 950 Degree C), Stainless Steel 310H Stub End Pipe Fittings is subject to sigma phase precipitation. Stainless Steel 310H End Cap Pipe Fittings contains 25 percent chromium and 20 percent nickel, making them highly resistant to oxidation and corrosion. Stainless Steel 310H Dish Cap Pipe Fittingsis often used in Furnace Parts, Heat Exchangers, and Oil Burner Parts. Stainless Steel 310H Lateral Tee Pipe Fittings has high temperature strength and good creep resistance. 310H Stainless Steel Pipe Fittings is widely used in moderately carburizing atmospheres such as encountered in petrochemical environments. Whilst retaining good strength when exposed to high temperatures, Stainless Steel UNS S31009 Pipe Fittings will also maintain its strength and toughness at sub-zero temperatures.
SS 310H Buttweld Pipe Fittings, SS 310H Long Stub bends, UNS S31009 Steel Elbow Supplier, 310H Steel Tee, SS 310H Pipe Cross, 310H Steel Reducers, Stainless Steel 310H Short Radius Elbow, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 310H Pipe Fittings Specifications
| Grade | SS 310H | UNS S31009 |
| Standard | ASTM A403 / ASME SA403 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| STANDARD | SS 310H |
| UNS | S31009 |
| WERKSTOFF NR. | - |
Stainless Steel 310H Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SS 310H | 0.04 – 0.10 | 2 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | – | 19.00 – 21.00 | 53.885 min |
Stainless Steel 310H Pipe Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40% |
Other Types of Stainless Steel 310H Pipe Fittings
- SS 310H Buttweld Tee Supplier in UAE
- Stainless UNS S31009 Cross Manufacturer in India
- SS 310H Butwteld Tee
- UNS S31009 45deg.Elbow
- S31009 Buttweld Pipe Fittings
- 310H Steel Short Radius Elbow
- UNS S31009 Ecentric Reducer Distributors
- SS 310H Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 310 Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 310H U Bend
- SS 310H Stub End Supplier in Poland
- 310H Short Radius Elbow
- WP 310H Steel Equal Tee in Qatar
- UNS S31009 End Cap
- ASME SA403 Concentric Reducer
- SS 310H Seamless Fitting
- Stainless Steel 310H 45 Elbow
- SS 310H Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 310H Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 310H Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo