Hastelloy C276 Pipe Fittings
UNS N10276 Hastelloy 90 Deg & 45 Deg Elbow, Hastelloy C276 Short Radius Elbow, ASME B16.28 Alloy C276 Long Radius Elbow, Hastelloy C276 Short & Long Stub End, ANSI B16.9 Alloy C276 Lateral Tee Manufacturer in Mumbai, India.
Nickel Super Alloys is a known supplier and exporter of Hastelloy Alloy C276 Butt Weld Pipe Fittings, which has outstanding resistance to all manner of pitting and cracking. Hastelloy C276 Elbow Pipe Fittings displays excellent resistance to pitting and crevice corrosion, SCC and oxidizing atmospheres up to 1040 Degree C. With an addition of tungsten, Hastelloy C276 Tee Pipe Fittings is designed to have excellent corrosion resistance in a wide range of severe environments. Hastelloy C276 Cross Pipe Fittings is widely accepted in the chemical process and associated industries. Hastelloy C276 Reducer Pipe Fittings is resistant to the formation of grain boundary precipitates in the weld heat-affected zone. Applications of Hastelloy C276 Bend Pipe Fittings include and are not limited to, ducts, dampers, stack liners, scrubbers, etc.
Like many other nickel alloys, Hastelloy C276 Stub End Pipe Fittings is ductile, easily formed and welded. The low carbon of Hastelloy C276 End Cap Pipe Fittings minimizes carbide precipitation duringwelding. Hastelloy C276 Dish Cap Pipe Fittings maintains resistance to inter-granular attack in heat effected zones of weld joints. Hastelloy C276 Lateral Tee Pipe Fittings has excellent corrosion resistance in both oxidizing and reducing environments. Hastelloy C276 Concentric Reducer Pipe Fittings is suitable for hot contaminated media, seawater and brine solutions,formic and acetic acids. Hastelloy C276 Eccentric Reducer Pipe Fittings should be considered for organic and inorganic chloride-contaminated media, formic and acetic acids, chlorine, acetic and acetic anhydride.
Hastelloy C276 Eccentric Reducer, Hastelloy Alloy C276 Pipe Bend, UNS N10276 End Cap & Dish Cap, Alloy C276 Concentric Reducer, Hastelloy Alloy C276 Equal Tee & Unequal Tee, Alloy C276 Fitting Cross Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy C276 Pipe Fittings Specifications
| Grade | Hastelloy Alloy C276 / UNS N10276 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Hastelloy C276 Seamless Fittings | 1/2" NB - 10" NB |
| Hastelloy C276 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Hastelloy C276 |
| EN | NiMo16Cr15W |
| UNS | N10276 |
| OR | ЭП760 |
| JIS | NW 0276 |
| GOST | ХН65МВУ |
| AFNOR | NFE30C20DUM |
| WERKSTOFF NR. | 2.4819 |
| BS | - |
Hastelloy C276 Pipe Fittings Chemical Composition
| Hastelloy C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balance | 0.01 max | 15 – 17 | 1.0 max | 0.08 max | 4 – 7 | 0.04 max | 0.03 max | 2.5 max | 14.5 – 16.5 |
Hastelloy C276 Pipe Fittings Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 52,000 , MPa – 355 | Psi – 1,15,000 , MPa – 790 | 40 % |
Other Types of Hastelloy C276 Pipe Fittings
- Hastelloy C276 Buttweld Tee Supplier in UAE
- UNS N10276 Cross Manufacturer in India
- DIN 2.4819 Butwteld Tee
- DIN 2.4819 45 deg.Elbow
- Hastelloy C276 Buttweld Pipe Fittings
- Hastelloy C276 Short Radius Elbow
- UNS N10276 Ecentric Reducer Distributors
- Hastelloy C276 Buttweld Pipe Fitting
- ASME SB366 Stub End
- C276 Hastelloy Concentric Reducer
- Hastelloy C276 Long Radius Elbow Exporter in Russia
- Hastelloy C22 U Bend
- Hastelloy C276 Stub End Supplier in Poland
- C276 Hastelloy Short Radius Elbow
- Hastelloy C276 Equal Tee in Qatar
- UNS N10276 End Cap
- ASME SB366 Concentric Reducer
- Hastelloy C276 Seamless Fitting
- Hastelloy C276 180 Deg Elbow
- Hastelloy C276 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy C276 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy C276 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo