Hastelloy B3 Pipe Fittings
Hastelloy B3 Pipe Elbow, Hastelloy 3D Pipe Bend, B3 Hastelloy Alloy Reducer, B3 Hastelloy Alloy End Cap, Hastelloy UNS N010675 Seamless Pipe Fittings, Hastelloy DIN 2.4600 Cross Manufacturer in Mumbai,India.
Nickel Super Alloys is a known manufacturer and supplier of Hastelloy Alloy B3 Butt Weld Pipe Fittings, which with stands wet hydrochloric gas, sulfuric and acetic acid. In addition, Hastelloy B3 Elbow Pipe Fittings has great resistance to knife-line and heat–affected zone attack. Furthermore, Hastelloy B3 Tee Pipe Fittingshas greatly improved structural stability compared with previous B-type alloys. Like other nickel alloys (in the mill annealed condition), Hastelloy B3 Cross Pipe Fittings is ductile, can be formed and welded. Hastelloy B3 Reducer Pipe Fittings has excellent resistance to pitting corrosion and to stress-corrosion cracking.
Hastelloy B3 Bend Pipe Fittings has a special chemistry designed to achieve a level of thermal stability greatly superior to that of its predecessors. The improved thermal stability of Hastelloy B3 Stub End Pipe Fittings minimizes the problems associated with fabrication of B-2 alloy components. Hastelloy B3 End Cap Pipe Fittingshas excellent resistance to pitting corrosion, to SCC and to knife-line and heat-affected zone attack. Hastelloy B3 Dish Cap Pipe Fittings should not be used in oxidizing media or in presence of oxidizing salts, such as cupric or ferric salts. The primary function of Hastelloy B3 Lateral Tee Pipe Fittings is to survive under high-stress and high-temperature applications. Hastelloy B3 Concentric Reducer Pipe Fittings is not recommended for use in oxidizing media or in the presence of ferric or cupric salts because they may cause rapid premature corrosion failure.
Alloy B3 Short & Long Radius Elbow, Hastelloy B3 180 Degree Elbow, ASTM B366 B3 Hastelloy Alloy 90 Degree Elbow, ASME SB366 Alloy B3 Long & Short Stub End, ANSI B16.9 Hastelloy B3 Eccentric & Concentric Reducer Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B3 Pipe Fittings Specifications
| Grade | Hastelloy Alloy B3 / UNS N10675 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Hastelloy B3 Seamless Fittings | 1/2" NB - 10" NB |
| Hastelloy B3 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Hastelloy B3 |
| UNS | N10675 |
| WERKSTOFF NR. | - |
Hastelloy B3 Pipe Fittings Chemical Composition
| Hastelloy B3 | Ni | C | Mo | Mn | Si | Fe | Cu | Ti | Co | Cr |
| 65.0 min | 0.01 max | 28.5 | 3.0 max | 0.10 max | 1.5 | 0.20 max | 0.2 max | 3.0 max | 1.5 |
Hastelloy B3 Pipe Fittings Mechanical Properties
| STANDARD | UNS | WERKSTOFF NR. |
| Hastelloy B3 | N010675 | 2.4600 |
Other Types of Hastelloy B3 Pipe Fittings
- Hastelloy B3 Buttweld Tee Supplier in UAE
- UNS N10675 Cross Manufacturer in India
- UNS N10675 Butwteld Tee
- UNS N10675 45 deg.Elbow
- Hastelloy B3 Buttweld Pipe Fittings
- Hastelloy B2 Short Radius Elbow
- UNS N10675 Ecentric Reducer Distributors
- Hastelloy B3 Buttweld Pipe Fitting
- ASME SB366 Stub End
- B3 Hastelloy Concentric Reducer
- Hastelloy B3 Long Radius Elbow Exporter in Russia
- Hastelloy B3 U Bend
- Hastelloy B3 Stub End Supplier in Poland
- B3 Hastelloy Short Radius Elbow
- Hastelloy B3 Equal Tee in Qatar
- UNS N10675 End Cap
- ASME SB366 Concentric Reducer
- Hastelloy B3 Seamless Fitting
- Hastelloy B3 180 Deg Elbow
- Hastelloy B3 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B3 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B3 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo