Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings
ANSI B16.11 SS 316 Threaded Street Elbows, Stainless Steel 316L Threaded Cap, Stainless Steel 316Ti Threaded Tee, ASME SA182M SS 316 Class 6000 Threaded Fittings Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the leading distributor and supplier of Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings, which is commonly used in the food industry. Stainless Steel 316 Threaded Forged Fittings has excellent formability and provides outstanding corrosion resistance. Stainless Steel 316L Threaded Elbow Forged Fittings is readily brake or roll formed into a variety of parts for applications. Stainless Steel 316Ti Threaded Tee Forged Fittings contains much higher chromium levels, and additional alloying ingredients. Stainless Steel 316 Threaded Cross Forged Fittings has chromium and molybdenum contents to suit the environment the alloy must endure. Stainless Steel 316L Threaded Cap Forged Fittings is used in severe settings, from polluted marine environments to areas with sub-zero temperatures.
The molybdenum makes Stainless Steel 316Ti Threaded Coupling Forged Fittings more resistant to pitting and crevice corrosion in chloride-contaminated media. The higher nickel and molybdenum content in Stainless Steel 316 Threaded Bend Forged Fittings allows it to demonstrate better overall corrosion resistant properties. Stainless Steel 316L Threaded Union Forged Fittings also offer higher creep, tensile strength and stress-to-rupture at elevated temperatures. Stainless Steel 316Ti Threaded Plug Forged Fittings is often used in food processing and pharmaceutical equipment, especially in potable water. Stainless Steel 316 Threaded Bushing Forged Fittings is extensively used in heavy gauge welded components. Stainless Steel 316L Threaded Hex PlusForged Fittings is also extensively used in the oil and gas and chemical industries.
Stainless Steel 316L Threaded Union, ANSI B16.11 SS 316Ti Threaded 90 Deg Elbows, Stainless Steel 316 Threaded Bend, SS 316L Hex Plug, Stainless Steel 316 Threaded Coupling, SS 316Ti Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings Specifications
| Grade | SS 316 / 316L | UNS S31600 / S31603 |
| Standard | ASTM A182 & ASME SA182 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | SS 316 | SS 316L |
| UNS | S31600 | S31603 |
| WERKSTOFF NR. | 1.4401 / 1.4436 | 1.4404 / 1.4435 |
| AFNOR | Z7CND17‐11‐02 | Z3CND17‐11‐02 / Z3CND18‐14‐03 |
| JIS | SUS 316 | SUS 316L |
| GOST | - | 03Ch17N14M3 / 03Ch17N14M2 |
| BS | 316S31 / 316S33 | 316S11 / 316S13 |
| EN | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
| SS 316 | 0.08 max | 2 max | 1.00 max | 0.045 max | 0.030 max | 16 – 18 | 2.0 – 3.0 | 11 – 14 | 67.845 min |
| SS 316L | 0.035 max | 2 max | 1.00 max | 0.045 max | 0.030 max | 16 – 18 | 2.0 – 3.0 | 10 – 14 | 68.89 min |
| SS 316TI | 0.08 max | 2 max | 0.75 max | 0.045 max | 0.030 max | 16.00 – 18.00 | 2.00 – 3.00 | 10.00 – 14.00 | 68.395 min |
Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.0 g/cm3 | 1399 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
Other Types of Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings
- Stainless Steel 316 Forged Elbow Supplier in UAE
- DIN 1.4401 / 1.4436 Equal Tee Manufacturer in India
- SS 316L Threaded Cross
- SS 316Ti Threaded Union
- UNS S31600 Hexagonal Plug
- UNS S31603 / S31635 Threaded Hex Plug
- DIN 1.4404 / 1.4435 45 Deg Threaded Elbow Distributors
- DIN 1.4401 / 1.4436 Threaded Bushing
- SS 316 Threaded Lateral Tee
- 316L Stainless Steel Threaded Cross
- ASME B16.11 SS 316 Threaded Coupling Exporter in Russia
- Stainless Steel 316L Threaded Tees
- SS 316Ti Threaded 45 deg Elbow Supplier in Poland
- UNS S31600 / S31603 Threaded 90 deg Elbow
- DIN 1.4404 / 1.4435 Threaded Cap in Qatar
- DIN 1.4401 / 1.4436 Threaded Bend Flanges
- SS 316Ti Threaded Union
- UNS S31600 Threaded Bushing
- UNS S31603 Lateral Tee
- Stainless Steel 316 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo