Nickel Alloy 200 Threaded Forged Fittings
Nickel Alloy 200 Forged Threaded 90 Deg. Elbow, Nickel Alloy 200 Threaded Tee, UNS N02200 Threaded Cross, DIN 2.4066 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the finest manufacturers of Nickel 200 Threaded Forged Fittings in India, which perform best in reducing environments. Nickel 200 Threaded Elbow Forged Fittings has good mechanical properties and excellent resistance to many corrosive environments. Nickel 200 Threaded Tee Forged Fittings is extremely resistance to caustic alkalis up to and including the molten state.Nickel 200 Threaded Cross Forged Fittings provides corrosion resistance in neutral to moderately reducing environments. Nickel 200 Threaded Cap Forged Fittings is limited to service at temperatures below 315 Degree C. The corrosion resistance of Nickel 200 Threaded Bend Forged Fittings makes it particularly useful for maintaining product purity. Nickel 200 Threaded Coupling Forged Fittings has high electrical and thermal conductivity.
Nickel 200 Threaded Union Forged Fittings is embrittled by inter-granular precipitates at temperatures of 600 Degree F to 1400 Degree F in many processes. Nickel 200 Threaded Bushing Forged Fittings has outstanding resistance to caustic alkalis up to and including the molten state. Nickel 200 Threaded Plug Forged Fittingshas low gas content and vapor pressure, along with high thermal and electrical conductivities. Applications of Nickel 200 Threaded Hex Plus Forged Fittings include aerospace and defense as well as food processing. Nickel 200 Threaded Hexagonal Plus Forged Fittings is resistant to various reducing chemicals & caustic alkalis. Nickel 200 Threaded Lateral Tee Forged Fittings has excellent resistance to most corrosive and caustic environments.
Nickel Alloy 200 Threaded Cap, Alloy 200 Threaded Bend, UNS N02200 Threaded Weld Cross, Nickel Alloy 200 Threaded Bushing, DIN 2.4066 Threaded Coupling, Nickel Alloy 200 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Nickel Alloy 200 Threaded Forged Fittings Specifications
| Grade | Nickel Alloy 200 | UNS N02200 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, 2000 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | Nickel 200 |
| UNS | N02200 |
| GOST | НП-2 |
| WERKSTOFF NR. | 2.4066 |
| BS | NA 11 |
| AFNOR | N-100M |
| EN | Ni 99.2 |
| JIS | NW 2200 |
Nickel Alloy 200 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
Nickel Alloy 200 Threaded Forged Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
Other Types of Nickel Alloy 200 Threaded Forged Fittings
- Nickel Alloy 200 Forged Elbow Supplier in UAE
- Nickel Alloy 200 Equal Tee Manufacturer in India
- Alloy 200 Threaded Cross
- UNS N02200 Threaded Union
- UNS N02200 Hexagonal Plug
- DIN 2.4066 Threaded Hex Plug
- DIN 2.4066 45 Deg Threaded Elbow Distributors
- Nickel 200 Threaded Bushing
- Nickel 200 Threaded Lateral Tee
- Nickel 200 Alloy Threaded Cross
- Nickel 200 Threaded Coupling Exporter in Russia
- Alloy 200 Threaded Tees
- UNS N02200 45 deg Elbow Supplier in Poland
- UNS N02200 Threaded 90 deg Elbow
- DIN 2.4066 Threaded Cap in Qatar
- DIN 2.4066 Threaded Bend Flanges
- Nickel Alloy 200 Threaded Union
- Alloy 200 Threaded Bushing
- Nickel Alloy 200 Lateral Tee
- Nickel Alloy 200 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Nickel Alloy 200 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Nickel Alloy 200 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo