Monel 400 Threaded Forged Fittings
Monel 400 Forged Threaded 90 Deg. Elbow, Monel 400 Threaded Tee, UNS N04400 Threaded Cross, DIN 2.4360 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the known suppliers of Monel Alloy 400 Threaded Forged Fittings, which is available at cost-effective rates to our clients. Monel 400 Threaded Elbow Forged Fittings is used extensively in (for pipe) piping. Monel 400 Threaded Cross Forged Fittings has excellent resistance to rapidly flowing brackish or seawater where cavitation and erosion resistance is necessary. Monel 400 Threaded Cap Forged Fittings exhibits characteristics like good weldability, good corrosion resistance, and high strength. Monel 400 Threaded Coupling Forged Fittings has excellent resistance to several corrosive environments. Monel 400 Threaded Bend Forged Fittings contains the same quantity of nickel and copper as is found in a naturally occurring nickel ore. Monel 400 Threaded Union Forged Fittings has good weldability and moderate to high strength.
Monel 400 Threaded Bushing Forged Fittings is an expensive alloy, and hence its use is limited to those applications where it cannot be replaced with cheaper alternatives. Monel 400 Threaded Plug Forged Fittingsis only hardenable through cold working, rather than heat treatment. The conventional machining techniques used on iron alloys may be used for Monel 400 Threaded Hexagonal PlusForged Fittings. With high nickel content, Monel 400 Threaded Tee Forged Fittings is immune to chloride-induced stress corrosion cracking. Monel UNS N04400 Threaded Lateral Tee Forged Fittings is quite soft at high temperatures and hence forging is a relatively simple process. Monel 400 Threaded Forged Fittings is used for offshore and marine applications and for chemical processing.
Monel 400 Threaded Cap, Alloy 400 Threaded Bend, UNS N04400 Threaded Weld Cross, Monel 400 Threaded Bushing, DIN 2.4360 Threaded Coupling, Monel 400 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Monel 400 Threaded Forged Fittings Specifications
| Grade | Monel 400 | UNS N04400 |
| Standard | ASTM B564 | ASME B564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, 4000 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| 400 | 2.4360 | N04400 | NW 4400 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
Monel 400 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| 400 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
Monel 400 Threaded Forged Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
Other Types of Monel 400 Threaded Forged Fittings
- Monel 400 Forged Elbow Supplier in UAE
- Monel 400 Equal Tee Manufacturer in India
- Monel 400 Threaded Cross
- UNS N04400 Threaded Union
- UNS N04400 Hexagonal Plug
- DIN 2.4360 Threaded Hex Plug
- DIN 2.4360 45 Deg Threaded Elbow Distributors
- Monel 400 Threaded Bushing
- Monel 400 Threaded Lateral Tee
- Alloy 400 Alloy Threaded Cross
- Monel 400 Threaded Coupling Exporter in Russia
- Alloy 400 Threaded Tees
- UNS N04400 45 deg Elbow Supplier in Poland
- UNS N04400 Threaded 90 deg Elbow
- DIN 2.4360 Threaded Cap in Qatar
- DIN 2.4360 Threaded Bend Flanges
- NU-30M Threaded Union
- Alloy 400 Threaded Bushing
- NiCu30Fe Lateral Tee
- NiCu30Fe Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Monel 400 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Monel 400 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo