Hastelloy C22 Threaded Forged Fittings
Hastelloy C22 Forged Threaded 90 Deg. Elbow, Hastelloy C22 Threaded Tee, UNS N06022 Threaded Cross, DIN 2.4602 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a known exporter and supplier of Hastelloy Alloy C22 Threaded Forged Fittings, which has better overall corrosion resistance. Hastelloy C22 Threaded Elbow Forged Fittings is suitable for most chemical process applications in the as-welded condition. Molybdenum in Hastelloy C22 Threaded Tee Forged Fittings enhances corrosion resistance in reducing environments. Hastelloy C22 Threaded Cross Forged Fittings can be used in some complicated environment or with many different manufacture target factory depend on the omnipotent performance. Hastelloy C22 Threaded Cap Forged Fittings minimizes the formation of intermetallic phases (mu phase), metallic carbides precipation at the grain boundaries. Hastelloy C22 Threaded Coupling Forged Fittings has the ideal resistance to the reducing and oxidizing environment encountered in the process.
The molybdenum and tungsten content in Hastelloy C22 Threaded Bend Forged Fittings give good resistance to reducing media. The chief attributes of Hastelloy C22 Threaded Union Forged Fittings are resistance to both oxidizing and non-oxidizing chemicals, and protection from pitting. Hastelloy C22 Threaded Bushing Forged Fittings, combined with its commercial availability, makes it an excellent choice for demanding specifications. Hastelloy C22 Threaded Plug Forged Fittings has shown an outstanding resistance to a wide range of chemicals, including chlorides, inorganic and organic solutions. Because of its resistibility, Hastelloy C22 Threaded Hexagonal Plus Forged Fittingscan be used where "upset" conditions are likely to occur. Hastelloy C22 Threaded Lateral Tee Forged Fittings has outstanding resistance to both reducing and oxidizing media.
Hastelloy C22 Threaded Cap, Alloy C22 Threaded Bend, UNS N06022 Threaded Weld Cross, Hastelloy C22 Threaded Bushing, DIN 2.4602 Threaded Coupling, Hastelloy C22 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy C22 Threaded Forged Fittings Specifications
| Grade | Hastelloy C22 | UNS N06022 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, C220 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | Hastelloy C22 |
| UNS | N06022 |
| WERKSTOFF NR. | 2.4602 |
| JIS | NW 6022 |
| EN | NiCr21Mo14W |
Hastelloy C22 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C22 | 0.010 max | 0.50 max | 0.08 max | 0.02 max | 2.50 max | 50.015 min* | 20.00 – 22.50 | 2.00 – 6.00 | 12.50 – 14.50 | 0.02 max |
Hastelloy C22 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45 % |
Other Types of Hastelloy C22 Threaded Forged Fittings
- Hastelloy C22 Forged Elbow Supplier in UAE
- Hastelloy C22 Equal Tee Manufacturer in India
- Hastelloy C22 Threaded Cross
- UNS N06022 Threaded Union
- UNS N06022 Hexagonal Plug
- DIN 2.4602 Threaded Hex Plug
- DIN 2.4602 45 Deg Threaded Elbow Distributors
- Hastelloy C22 Threaded Bushing
- Hastelloy C22 Threaded Lateral Tee
- Alloy C22 Alloy Threaded Cross
- Hastelloy C22 Threaded Coupling Exporter in Russia
- Alloy C22 Threaded Tees
- UNS N06022 45 deg Elbow Supplier in Poland
- UNS N06022 Threaded 90 deg Elbow
- DIN 2.4602 Threaded Cap in Qatar
- DIN 2.4602 Threaded Bend Flanges
- Hastelloy C22 Threaded Union
- Alloy C22 Threaded Bushing
- Hastelloy C22 Lateral Tee
- Hastelloy C22 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy C22 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy C22 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo