Hastelloy B2 Threaded Forged Fittings
Hastelloy B2 Forged Threaded 90 Deg. Elbow, Hastelloy B2 Threaded Tee, UNS N10665 Threaded Cross, DIN 2.4617 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the known supplier and exporter of Hastelloy Alloy B2 Threaded Forged Fittings, which has poor resistance to oxidizing environments. Molybdenum in Hastelloy B2 Threaded Elbow Forged Fittings is the primary alloying element which provides significant corrosion resistance to reducing environments. Hastelloy B2 Threaded Tee Forged Fittings should not be used in oxidizing media or where oxidizing contaminants are available in reducing media. Hastelloy B2 Threaded Cross Forged Fittingsfeatures hydrochloric acid resistance at all concentrations and temperatures. Hastelloy B2 Threaded Cap Forged Fittings is less susceptible to decreased corrosion resistance in the weld zone, in the as-welded condition. Hastelloy B2 Threaded Coupling Forged Fittings is suitable for most chemical process conditions in the as-welded condition.
Hastelloy B2 Threaded Bend Forged Fittings is normally used in extreme reducing conditions. Hastelloy B2 Threaded Union Forged Fittings has excellent resistance to medium-concentrated sulfuric acid and a number of non-oxidizing acids. Hastelloy B2 Threaded Bushing Forged Fittings is not susceptible to grain-boundary carbide precipitation following welding. Other alloying ingredients are added to Hastelloy B2 Threaded Plug Forged Fittings including varying percentages of the elements molybdenum and chromium. Hastelloy B2 Threaded Hexagonal Plus Forged Fittings has outstanding corrosion resistance in the as-welded condition. Hastelloy B2 Threaded Lateral Tee Forged Fittings can function at very high temperatures and in severe mechanical stress environments, and also where high surface stability is required. Hastelloy UNS N10665 Threaded Forged Fittings has significantly lower carbon, silicon and iron compared to its’ predecessor.
Hastelloy B2 Threaded Cap, Alloy B2 Threaded Bend, UNS N10665 Threaded Weld Cross, Hastelloy B2 Threaded Bushing, DIN 2.4617 Threaded Coupling, Hastelloy B2 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B2 Threaded Forged Fittings Specifications
| Grade | Hastelloy B2 | UNS N10665 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, B20 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
Hastelloy B2 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| B2 | 0.01 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.0 – 17.0 | 0.04 max |
Hastelloy B2 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52000 , MPa – 355 | 40 % |
Other Types of Hastelloy B2 Threaded Forged Fittings
- Hastelloy B2 Forged Elbow Supplier in UAE
- Hastelloy B2 Equal Tee Manufacturer in India
- Hastelloy B2 Threaded Cross
- UNS N10665 Threaded Union
- UNS N10665 Hexagonal Plug
- DIN 2.4617 Threaded Hex Plug
- DIN 2.4617 45 Deg Threaded Elbow Distributors
- Hastelloy B2 Threaded Bushing
- Hastelloy B2 Threaded Lateral Tee
- Alloy B2 Alloy Threaded Cross
- Hastelloy B2 Threaded Coupling Exporter in Russia
- Alloy B2 Threaded Tees
- UNS N10665 45 deg Elbow Supplier in Poland
- UNS N10665 Threaded 90 deg Elbow
- DIN 2.4617 Threaded Cap in Qatar
- DIN 2.4617 Threaded Bend Flanges
- Hastelloy B2 Threaded Union
- Alloy B2 Threaded Bushing
- Hastelloy B2 Lateral Tee
- Hastelloy B2 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B2 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B2 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo