Monel K500 Threaded Forged Fittings
Monel K500 Forged Threaded 90 Deg. Elbow, Monel K500 Threaded Tee, UNS N05500 Threaded Cross, DIN 2.4375 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is of the well-known traders of Monel Alloy K500 Threaded Forged Fittings, which is often used in Electronic components, Valve trim, Springs, and more. Monel K500 Threaded Elbow Forged Fittings brings characteristics similar to Alloy 400 in respect to corrosion resistance. Monel K500 Threaded Tee Forged Fittings is often utilized in high-velocity seawater and in stagnant or slow-moving seawater. Monel K500 Threaded Cross Forged Fittings provides excellent corrosion resistance in a range of environments. Small additions of aluminum and titanium form Monel K500 Threaded Cap Forged Fittings with the same corrosion resistance but with much greater strength due to gamma prime formation on aging. Monel K500 Threaded Coupling Forged Fittings has excellent mechanical properties from sub-zero temperatures up to about 480 Degree C.
Monel K500 Threaded Bend Forged Fittings has excellent corrosion resistance in an extensive range of natural and chemical environments. When in the age-hardened condition, Monel K500 Threaded Union Forged Fittingshas a greater tendency toward stress-corrosion cracking in some environments. The addition of aluminum and titanium in Monel K500 Threaded Bushing Forged Fittings to an already robust nickel-copper base adds strength and hardness. Hot working of Monel K500 Threaded Plug Forged Fittings should be performed at temperatures between 1600 Degree F and 2100 Degree F avoiding any prolongs soaking time at the higher temperatures. Heat treatment of Monel K500 Threaded Lateral Tee Forged Fittings may involve solution and process annealing, followed by age hardening.
Monel K500 Threaded Cap, Alloy K500 Threaded Bend, UNS N05500 Threaded Weld Cross, Monel K500 Threaded Bushing, DIN 2.4375 Threaded Coupling, Monel K500 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Monel K500 Threaded Forged Fittings Specifications
| Grade | Monel K500 | UNS N05500 |
| Standard | ASTM B564 | ASME B564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, 4000 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel K500 | 2.4375 | N05500 | - | - | - | - | - |
Monel K500 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| K500 | 0.25 max | 1.5 max | 0.5 max | 0.010 max | 27.00 – 33.00 | 0.5 – 2 | 63.00 min |
Monel K500 Threaded Forged Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| K500 | 8.44 g/cm3 | 1350 °C (2460 °F) | Psi – 160000 , MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |
Other Types of Monel K500 Threaded Forged Fittings
- Monel K500 Forged Elbow Supplier in UAE
- Monel K500 Equal Tee Manufacturer in India
- Monel K500 Threaded Cross
- UNS N05500 Threaded Union
- UNS N05500 Hexagonal Plug
- DIN 2.4375 Threaded Hex Plug
- DIN 2.4375 45 Deg Threaded Elbow Distributors
- Monel K500 Threaded Bushing
- Monel K500 Threaded Lateral Tee
- Alloy K500 Alloy Threaded Cross
- Monel K500 Threaded Coupling Exporter in Russia
- Alloy K500 Threaded Tees
- UNS N05500 45 deg Elbow Supplier in Poland
- UNS N05500 Threaded 90 deg Elbow
- DIN 2.4375 Threaded Cap in Qatar
- DIN 2.4375 Threaded Bend Flanges
- Monel K500 Threaded Union
- Alloy K500 Threaded Bushing
- Monel K500 Lateral Tee
- Monel K500 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Monel K500 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Monel K500 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo