Incoloy 925 Threaded Forged Fittings
Incoloy 925 Forged Threaded 90 Deg. Elbow, Incoloy 925 Threaded Tee, ASTM B564 Incoloy 925 Threaded Cross, UNS N09925 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the leading names in manufacturing Inconel Alloy 925 Threaded Forged Fittings, which is age hardenable nickel iron chromium alloy. Inconel 925 Threaded Elbow Forged Fittings has excellent corrosion resistance consistent with Alloy 825. The molybdenum in Inconel 925 Threaded Tee Forged Fittings aids with the resistance to pitting and crevice corrosion. Inconel 925 Threaded Cross Forged Fittings is one of four elements that are ferromagnetic. The nickel content in Inconel 925 Threaded Cap Forged Fittingsis sufficient for protection against chloride-ion SCC. Inconel 925 Threaded Coupling Forged Fittings is resistance to chloride ion stress-corrosion cracking. Inconel 925 Threaded Bend Forged Fittings is used in the petroleum industry for applications such as gas well components.
Inconel 925 Threaded Union Forged Fittings is used in many aqueous environments including those containing sulfides and chlorides. Inconel 925 Threaded Plug Forged Fittings can also be used for fasteners, and for pump shafts in marine environments. In conjunction with the added molybdenum and copper, resistance in Inconel 925 Threaded Bushing Forged Fittings to reducing chemicals is enjoyed. Inconel 925 Threaded Hexagonal Plus Forged Fittings can be used in environments with high temperatures and mechanical stress. Inconel 925 Threaded Lateral Tee Forged Fittingshas excellent resistance to pitting and crevice corrosion. Inconel 925 Threaded Hex Plus Forged Fittingsis particularly resistant to sulfide-induced stress cracking and stress-corrosion cracking.
ASME SB564 Incoloy 925 Threaded Cap, Incoloy 925 Threaded Bend, UNS N09925 Threaded Weld Cross, Incoloy 925 Threaded Bushing, Incoloy 925 Threaded Coupling, Incoloy 925 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 925 Threaded Forged Fittings Specifications
| Grade | Incoloy 925 | UNS N09925 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, 9250 LBS, 9000 LBS |
| Form | Threaded weld 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Incoloy 925 |
| UNS | N09925 |
| WERKSTOFF NR. | - |
Incoloy 925 Threaded Forged Fittings Chemical Composition
| Grade | Ni | Cr | Fe | Si | Mo | Cu | Mn | C | S | Al |
| Incoloy 925 | 42 – 46 | 19.55 – 22.5 | 22 min | 0.5 max | 2.5 – 3.5 | 1.5 – 3.0 | 1.0 max | 0.03 max | 0.03 max | 0.1 – 0.5 |
Incoloy 925 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.14 g/cm3 | 1343°C | 650 | 300 | 30 % |
Other Types of Incoloy 925 Threaded Forged Fittings
- Incoloy 925 Forged Elbow Supplier in UAE
- Incoloy 925 Equal Tee Manufacturer in India
- Incoloy 925 Threaded Cross
- Incoloy 925 Threaded Union
- UNS N09925 Hexagonal Plug
- UNS N09925 Threaded Hex Plug
- Incoloy 925 45 Deg Threaded Elbow Distributors
- Incoloy 925 Threaded Bushing
- Incoloy 925 Threaded Lateral Tee
- Incoloy 925 Alloy Threaded Cross
- Incoloy 925 Threaded Coupling Exporter in Russia
- Incoloy 925 Threaded Tees
- Incoloy 925 45 deg Elbow Supplier in Poland
- Incoloy 925 Threaded 90 deg Elbow
- Incoloy 925 Threaded Cap in Qatar
- Incoloy 925 Threaded Bend Flanges
- Incoloy 925 Threaded Union
- Incoloy 925 Threaded Bushing
- Incoloy 925 Lateral Tee
- Incoloy 925 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 925 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 925 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo