Alloy Steel F91 Threaded Forged Fittings
F91 Chrome Moly Forged Threaded 90 Deg. Elbow, Alloy Steel F91 Threaded Tee, ASME SA182M Alloy Steel F91 Threaded Cross, F91 Chrome Moly Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a well-known manufacturer of Alloy Steel F91 Threaded Forged Fittings, which have good weldability by all conventional processes. Manufactured using optimum quality raw material at our ends, these Alloy Steel F91 Threaded Elbow Forged Fittingsare appreciated and demanded by the clients for their strength, corrosion resistance and superior finish. In the run of becoming the best name of the industry, we are engaged in offering Alloy Steel F91 Threaded Tee Forged Fittingsthat we offer are highly appreciated in the industry for its thermal resistant in nature. Our company has mastered the art in offering Alloy Steel F91 Threaded Cross Forged Fittings to the clients, which is manufactured using highest grade raw material by our trusted experts of the market.
We also ensure these Alloy Steel F91 Threaded Cap Forged Fittings are made available in eye-catching finish looks, corrosion resistant finish, needing low maintenance requirements as well as delivering long service support as desired by the customers. Besides, one can get these Alloy Steel F91 Threaded Bend Forged Fittings at industry leading prices. These Alloy Steel F91 Threaded Coupling Forged Fittings are appreciated across the nation for reliability, consistency and easy installation. Alloy Steel F91 Threaded Union Forged Fittings appear to be slightly oxidized and have been bought by many of our customers. Alloy Steel F91 Threaded Bushing Forged Fittings can be supplied in bulk quantity as well as retail quantity as per customers’ requirements.
ASTM A182 Alloy Steel F91 Threaded Cap, ASME 16.11 Alloy Steel F91 Threaded Bend, Alloy Steel F91 Threaded Weld Cross, Alloy Steel F91 Threaded Bushing, F91 Alloy Steel Threaded Coupling, Alloy Steel F91 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Alloy Steel F91 Threaded Forged Fittings Specifications
| Grade | Alloy Steel Grade F91 |
| Standard | ASTM A182, ASME SA182 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | F910 LBS, 3000 LBS, F910 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
Alloy Steel F91 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | P | Cr | Mo |
| Alloy Steel F91 | 0.08-0.12 | 0.3-0.6 | 0.5 | 0.01 | 0.02 | 8.5-9.5 | 0.85-1.05 |
Alloy Steel F91 Threaded Forged Fittings Mechanical Properties
| Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 415 | 585 | 20 % |
Other Types of Alloy Steel F91 Threaded Forged Fittings
- Alloy Steel F91 Forged Elbow Supplier in UAE
- Gr F91 Alloy Equal Tee Manufacturer in India
- Alloy Steel F91 Threaded Cross
- Alloy Steel F91 Threaded Union
- F91 Chrome Moly Hexagonal Plug
- F91 Chrome Moly Threaded Hex Plug
- Alloy Steel F91 45 Deg Threaded Elbow Distributors
- Alloy Steel F91 Threaded Bushing
- Grade F91 Alloy Threaded Lateral Tee
- Grade F91 Alloy Threaded Cross
- Alloy Steel F91 Threaded Coupling Exporter in Russia
- Alloy Steel F91 Threaded Tees
- Gr F91 Alloy Threaded 45 deg Elbow Supplier in Poland
- Gr F91 Alloy Threaded 90 deg Elbow
- F91 Chrome Moly Threaded Cap in Qatar
- F91 Chrome Moly Threaded Bend Flanges
- Alloy Steel F91 Threaded Union
- Alloy Steel F91 Threaded Bushing
- Alloy Steel F91 Lateral Tee
- Alloy Steel F91 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Alloy Steel F91 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Alloy Steel F91 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo