Inconel 625 Socket Weld Forged Fittings
Inconel 625 Socket Weld 90 Deg. Elbow, Inconel 625 Socket Weld Tee, UNS N06625 Socket Weld Cross, DIN NR. 2.4856 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the finest supplier and exporter of Inconel Alloy 625 Socket Weld Forged Fittings, which has excellent weldability. Rapid changes in temperature (which are common in heat treat applications) are not as much of an issue for Inconel 625 Socket Weld Elbow Forged Fittings. Some typical applications for Inconel 625 Socket Weld Tee Forged Fittings have included heat shields and furnace hardware. Inconel 625 Socket Weld Cap Forged Fittings has excellent fabricability and outstanding corrosion resistance. Inconel 625 Socket Weld Cross Forged Fittings is especially resistant to pitting and crevice corrosion. Inconel 625 Socket Weld Coupling Forged Fittingsis good for sea water applications.
Inconel 625 Socket Weld Union Forged Fittings is used for pressure vessels in a temperature range from -196 Degree C to 450 Degree C. Inconel 625 Socket Weld Plug Forged Fittings has ability to withstand high stress and a wide range of temperatures, both in and out of water. Inconel 625 Socket Weld Lateral Tee Forged Fittings acts with the molybdenum to stiffen the alloy’s matrix. Nickel Alloy 625 Socket Weld Forged Fittings allows maintaining high strength and toughness at temperatures ranging from cryogenic up to 2000 Degree F (1093 Degree C). Inconel UNS N06625 Socket Weld Forged Fittings has outstanding resistance to crevice corrosion, pitting, and inter-crystalline corrosion. Inconel WNR 2.4856 Socket Weld Forged Fittings has highly alloyed composition also provides a significant level of general corrosion resistance.
Inconel 625 Socket Weld Cap, Inconel 625 Socket Weld Bend, Inconel 625 Socket Weld Cross, Inconel 625 Socket Weld Bushing, UNS N06625 Socket Weld Coupling, ASTM B564 Inconel 625 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Inconel 625 Socket Weld Forged Fittings Specifications
| Grade | Inconel Alloy 625 | UNS N06625 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, 6250 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Inconel 625 |
| UNS | N06625 |
| GOST | ХН75МБТЮ |
| BS | NA 21 |
| AFNOR | NC22DNB4M |
| JIS | NCF 625 |
| EN | NiCr22Mo9Nb |
| WERKSTOFF NR. | 2.4856 |
| OR | ЭИ602 |
Inconel 625 Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Cu | Ni | Fe |
| Inconel 625 | 0.10 max | 0.50 max | 0.5 max | – | 0.015 max | 20.0 – 23.0 | – | 58 min | 5.0 max |
Inconel 625 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.4 g/cm3 | 1350 °C (2460 °F) | Psi – 1,35,000 , MPa – 930 | Psi – 75,000 , MPa – 517 | 42.5 % |
Other Types of Inconel 625 Socket Weld Threaded Forged Fittings
- Inconel 625 Socket Weld Forged Elbow Supplier in UAE
- Inconel 625 Socket Weld Equal Tee Manufacturer in India
- Inconel 625 Socket Weld Cross
- Inconel 625 Socket Weld Union
- UNS N06625 Socket Weld Plug
- UNS N06625 Socket Weld Hex Plug
- DIN NR. 2.4856 45 Deg Socket Weld Elbow Distributors
- DIN NR. 2.4856 Socket Weld Bushing
- Inconel 625 Socket Weld Lateral Tee
- Inconel 625 Socket Weld Cross
- Inconel 625 Socket Weld Coupling Exporter in Russia
- Inconel 625 Socket Weld Tees
- UNS N06625 45 deg Socket Weld Elbow Supplier in Poland
- UNS N06625 Socket Weld 90 deg Elbow
- DIN NR. 2.4856 Socket Weld Cap in Qatar
- DIN NR. 2.4856 Socket Weld Bend Flanges
- NiCr22Mo9Nb Socket Weld Union
- NC22DNB4M Socket Weld Bushing
- ХН75МБТЮ Socket Weld Lateral Tee
- Inconel 625 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Inconel 625 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Inconel 625 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo