Incoloy 925 Socket Weld Forged Fittings
Incoloy 925 Socket Weld 90 Deg. Elbow, Incoloy 925 Socket Weld Tee, UNS N09925 Socket Weld Cross, Incoloy 925 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the leading names in manufacturing Inconel Alloy 925 Socket Weld Forged Fittings, which has excellent resistance to pitting and crevice corrosion. Inconel 925 Socket Weld Elbow Forged Fittingsis an age hardenable nickel based alloy that contains chromium and iron as important ingredients. Inconel 925 Socket Weld Tee Forged Fittings is used in air and vacuum melting, vacuum arc and electroslag re-melting. The chemical composition in Inconel 925 Socket Weld Cap Forged Fittings is designed to provide a combination of high strength and excellent corrosion resistance. The chromium content in Inconel 925 Socket Weld Cross Forged Fittings provides resistance to oxidizing environments.
Inconel 925 Socket Weld Coupling Forged Fittings is used in the production of various types of magnets for commercial use. The nickel in Inconel 925 Socket Weld Union Forged Fittings, in conjunction with the molybdenum and copper, also gives outstanding resistance to reducing chemicals. Inconel 925 Socket Weld Plug Forged Fittings is used for valves and tubing, as well as finding use in high-strength piping systems. Inconel 925 Socket Weld Lateral Tee Forged Fittings is used for surface and down-hole hardware in sour gas wells and for oil-production equipment. The combination of Nickel and Chromium in Inconel UNS N09925 Socket Weld Forged Fittings renders protection in both oxidizing and reducing atmospheres. Nickel-Alloy 925 Socket Weld Forged Fittings has high levels of nickel ensure protection against stress corrosion cracking.
Incoloy 925 Socket Weld Cap, Incoloy 925 Socket Weld Bend, Incoloy 925 Socket Weld Cross, Incoloy 925 Socket Weld Bushing, UNS N09925 Socket Weld Coupling, ASTM B564 Incoloy 925 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 925 Socket Weld Forged Fittings Specifications
| Grade | Incoloy 925 | UNS N09925 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, 9250 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Incoloy 925 |
| UNS | N09925 |
| WERKSTOFF NR. | - |
Incoloy 925 Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | Al | S | Cr | Cu | Ni | Fe |
| Incoloy 925 | 0.03 max | 1.0 max | 0.5 max | 0.01-0.05 | 0.03 max | 19.55-22.50 | 1.50-3.00 | 42.0-46.0 | 22 min |
Incoloy 925 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.14 g/cm3 | 1343 °C | MPa – 650 | MPa – 300 | 30 % |
Other Types of Incoloy 925 Socket Weld Threaded Forged Fittings
- Incoloy 925 Socket Weld Forged Elbow Supplier in UAE
- Incoloy 925 Socket Weld Equal Tee Manufacturer in India
- Incoloy 925 Socket Weld Cross
- Incoloy 925 Socket Weld Union
- UNS N09925 Socket Weld Plug
- UNS N09925 Socket Weld Hex Plug
- Incoloy 925 45 Deg Socket Weld Elbow Distributors
- Incoloy 925 Socket Weld Bushing
- Incoloy 925 Socket Weld Lateral Tee
- Incoloy 925 Socket Weld Cross
- Incoloy 925 Socket Weld Coupling Exporter in Russia
- Incoloy 925 Socket Weld Tees
- UNS N09925 45 deg Socket Weld Elbow Supplier in Poland
- UNS N09925 Socket Weld 90 deg Elbow
- Incoloy 925 Socket Weld Cap in Qatar
- Incoloy 925 Socket Weld Bend Flanges
- Incoloy 925 Socket Weld Union
- Incoloy 925 Socket Weld Bushing
- Incoloy 925 Socket Weld Lateral Tee
- Incoloy 925 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 925 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 925 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo