Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings
Incoloy 800 Socket Weld 90 Deg. Elbow, Incoloy 800HT Socket Weld Tee, UNS N08800 / N08810 Socket Weld Cross, DIN NR. 1.4876 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of leading distributors and suppliers of Inconel Alloy 800 / 800H / 800HT Socket Weld Forged Fittings, which is a solution heat treated. Inconel 800 Socket Weld Elbow Forged Fittings is readily machined by standard methods. Inconel 800 Socket Weld Tee Forged Fittings is extremely resistant to corrosion, even in acidic environment. Inconel 800 Socket Weld Cap Forged Fittings also resists corrosion in many aqueous environments. Inconel 800 Socket Weld Cross Forged Fittings has good creep-rupture properties at temperatures above 1100 Degree F (600 Degree C).Inconel 800 Socket Weld Coupling Forged Fittings offers a closer match of thermal expansion coefficient, and somewhat higher strength.
High nickel and chromium contents in Inconel 800 Socket Weld Union Forged Fittings result in excellent resistance to oxidation, carburization and suffixation. The nickel content makes Inconel 800 Socket Weld Plug Forged Fittings highly resistant to both chloride SCC and to embrittlement from precipitation of sigma phase. Inconel 800 Socket Weld Lateral Tee Forged Fittings is meant to fill the need for a heat and corrosion-resistant alloy with relatively low nickel content. Inconel UNS N08800 Socket Weld Forged Fittings has excellent resistance to chloride stress-corrosion cracking. Inconel UNS N08810 Socket Weld Forged Fittings doesn't form the embrittling sigma phase after long time exposure at 1200 Degree F. Other characteristics of Inconel UNS N08811 Socket Weld Forged Fittings are good strength, and high resistance to reducing,oxidizing, and aqueous environments.
Incoloy 800 Socket Weld Cap, Incoloy 800H Socket Weld Bend, Incoloy 800HT Socket Weld Cross, Incoloy 800 Socket Weld Bushing, UNS N08811 Socket Weld Coupling, ASTM B564 Incoloy 800HT Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings Specifications
| Grade | Incoloy Alloy 800 / 800H / 800HT | UNS N08800 / N08810 / N08811 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, 8000 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Incoloy 800 | Incoloy 800H | Incoloy 800HT |
| UNS | N08800 | N08810 | N08811 |
| EN | X10NiCrAlTi32-20 | X5NiCrAlTi31-20 | X8NiCrAlTi32-21 |
| AFNOR | Z8NC32-21 | Z8NC33-21 | - |
| JIS | NCF 800 | NCF 800H | NCF 800HT |
| BS | NA 15 | NA 15(H) | NA 15(HT) |
| WERKSTOFF NR. | 1.4876 | 1.4958 / 1.4876 | 1.4859 / 1.4876 |
| GOST | ЭИ670 | ЭИ670 | ЭИ670 |
| OR | XH32T | XH32T | XH32T |
Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | Al | S | Cr | Cu | Ni | Fe |
| Incoloy 800 | 0.10 max | 1.50 max | 1 max | 0.15 – 0.60 | 0.015 max | 19.0-23.0 | 0.75 max | 30.0-35.0 | 39.5 min |
| Incoloy 800H | 0.05 – 0.10 | 1.50 max | 1 max | 0.15 – 0.60 | 0.015 max | 19.0-23.0 | 0.75 max | 30.0-35.0 | 39.5 min |
| Incoloy 800HT | 0.06 – 0.10 | 1.50 max | 1 max | 0.15 – 0.60 | 0.015 max | 19.0-23.0 | 0.75 max | 30.0-35.0 | 39.5 min |
Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1385 °C (2525 °F) | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa – 205 | 30 % |
Other Types of Incoloy 800 / 800H / 800HT Socket Weld Threaded Forged Fittings
- Incoloy 800 Socket Weld Forged Elbow Supplier in UAE
- Incoloy 800H Socket Weld Equal Tee Manufacturer in India
- Incoloy 800 Socket Weld Cross
- Incoloy 800HT Socket Weld Union
- UNS N08800 / N08810 Socket Weld Plug
- UNS N08811 Socket Weld Hex Plug
- DIN NR. 1.4876 45 Deg Socket Weld Elbow Distributors
- DIN NR. 1.4958 / 1.4876 Socket Weld Bushing
- Incoloy 800 Socket Weld Lateral Tee
- Incoloy 800H Socket Weld Cross
- Incoloy 800 Socket Weld Coupling Exporter in Russia
- Incoloy 800H Socket Weld Tees
- UNS N08800 45 deg Socket Weld Elbow Supplier in Poland
- UNS N08810 / N08811 Socket Weld 90 deg Elbow
- DIN NR. 1.4859 / 1.4876 Socket Weld Cap in Qatar
- DIN NR. 1.4958 / 1.4876 Socket Weld Bend Flanges
- X10NiCrAlTi32-20 Socket Weld Union
- X5NiCrAlTi31-20 Socket Weld Bushing
- X8NiCrAlTi32-21 Socket Weld Lateral Tee
- Incoloy 800 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 800 / 800H / 800HT Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo