Hastelloy B3 Flanges
Alloy B3 SORF Flange, ANSI B16.5 Alloy B3 Orifice Flange, Alloy B3 RTJ Flange, Hastelloy B3 Spectacle Blind Flanges, Hastelloy B3 Pipe Flanges Manufacturer in Mumbai,India.
Nickel Super Alloys is a known manufacturer and supplier of Hastelloy Alloy B3 Pipe Flanges, which has poor corrosion resistance to oxidizing environments. The attributes of Corrosion-Resistant Hastelloy B3 Slip On Raised Flanges include high resistance to uniform attack. Hastelloy B3 Blind Raised Flanges has excellent resistance to hydrochloric acid at all concentrations and temperatures. Hastelloy B3 Spectacle Blind Flanges is used in the construction of reaction vessels for pure, reducing acid service. The molybdenum content of Hastelloy B3 Threaded Flanges is such that there is a strong tendency for phases other than the desirable (face-centered cubic) gamma phase to form in the microstructure. Hastelloy B3 Socket Weld Flangeshas excellent resistance to pitting corrosion & stress corrosion cracking.
Hastelloy B3 Weld Neck Flanges has greater ductility than B2 alloy during and following various thermal cycling conditions. Hastelloy B3 Lap Joint Flanges is used for deep drawn parts and those parts that need to retain lubricants in the forming process. Hastelloy B3 Ring Joint Type Flangeshas superior thermal stability to the B-2 alloy because of judicious use of minor elements and a shift in the molybdenum content. Hastelloy B3 Spacer Flanges maintains excellent ductility during transient exposures to intermediate temperatures. Hastelloy B3 Long Weld Neck Flanges gives outstanding resistance to non-oxidizing acids at the whole magnitudes and temperature limits. Hastelloy B3 Nippolet Flanges may be forged or otherwise hot-worked.
Hastelloy B3 Slip On Flanges, Hastelloy B3 Nippo Flanges, Hastelloy DIN 2.4600 Socket Weld Flanges, Hastelloy B3 Slip On Flanges, Hastelloy UNS N010675 Socket Weld Flanges, ANSI B16.5 Alloy B3 Orifice Flange, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B3 Flanges Specifications
| Grade | Hastelloy Alloy B3 / UNS N10675 |
| Standard | ASTM B564, ASME SB564 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, B3 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| Standard | Hastelloy B3 |
| UNS | N10675 |
| WERKSTOFF NR. | - |
Hastelloy B3 Flanges Chemical Composition
| Grade | Ni | Mo | Cr | Fe | W | Mn | C | Al | Ti | Si |
| Hastelloy B3 | 65.0 min | 28.5 | 1.5 | 1.5 | 3.0 max | 3.0 max | 0.01 max | 0.50 max | 0.2 max | 10 max |
Hastelloy B3 Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 9.2 g/cm3 | 1370 °C (2550 °F) | Psi – 1,15,000 , MPa –760 | Psi – 52,000 , MPa – 350 | 40% |
Other Types of Hastelloy B3 Flanges
- Hastelloy B3 Tongue & Groove Flanges Supplier in UAE
- Hastelloy B3 Spectacle blind flanges Manufacturer in India
- Hastelloy B3 Long Weld Neck Flanges
- Hastelloy B3 Flat Face Flanges
- UNS N10675 High Hub Blind Flanges
- UNS N10675 Lap Joint Flanges
- DIN 2.4600 Reducing Flanges Distributors
- DIN 2.4600 Blind Flanges
- Hastelloy B3 Slip On Flanges
- UNS N010675 Threaded Flanges
- Hastelloy B3 Orifice Flanges Exporter in Russia
- Hastelloy B3 400# Forged Flanges
- Hastelloy B3 F91 600# Plate Flanges Supplier in Poland
- Hastelloy B3 900# Spacer Ring Flanges
- DIN 2.4600 PN6 Nipo Flange in Qatar
- DIN 2.4600 PN10 Nipolet Flanges
- Hastelloy B3 Pipe Flanges
- UNS N010675 SORF Flanges
- Hastelloy B3 WNRF Flanges
- Hastelloy B3 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B3 Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B3 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo