Copper Nickel 90 / 10 Flanges
Cupro Nickel 90/10 RTJ Flange, Cupro Nickel Werkstoff No 2.0872 Socket Weld Flanges, 90/10 Cu-Ni WNRF Flanges, Cu-Ni 90/10 Blind Flanges, Cupro Nickel 90/10 Weld Neck Flange Manufacturer in Mumbai, India.
Nickel Super Alloys is a renowned distributor of Copper Nickel 90 / 10 Flanges, which enhance overall strength and corrosion resistance. The company has experience in these areas and is able to supply these Cupro Nickel 90 / 10 Slip On Raised Flanges in accordance with most international standards and special customer requirements. Cu-Ni 90 / 10 Blind Raised Flanges are extremely versatile known for its ductility, high heat transfer, and corrosion resistance. Due to the addition of small amounts of iron and manganese, Copper Nickel 90 / 10 Spectacle Blind Flanges is often used when an application will involve high-velocity seawater.
Cupro Nickel 90 / 10 Threaded Flanges have the retention of mechanical properties down to cryogenic temperatures. The resistance to soil erosion and abrasive fluids in Cu-Ni 90 / 10 Weld Neck Flanges is incomparable in the aqueous conditions. The cast structures of Copper Nickel 90 / 10 Socket Weld Flanges have alpha dendrites that contain huge quantities of nickel. Cupro Nickel 90 / 10 Lap Joint Flanges offers the best resistance to aqueous corrosion.Cu-Ni90 / 10 Ring Joint Type Flanges are used for marine applications due to their resistance to seawater corrosion. Copper Nickel 90 / 10 Spacer Flanges were developed specifically for seawater service, initially for condensers and piping systems. Cupro Nickel 90 / 10 Nippolet Flanges resists attack by sulfuric, phosphoric, and mild organic acids.
ASTM A151 Cu-Ni 90/10 Threaded Flanges, Copper Nickel UNS C70600 Pipe Flanges, ANSI B16.5 Cupro Nickel 90/10 Orifice Flange, Cupro Nickel 90/10 Slip On Flanges, Cupro Nickel 90/10 Nippo Flanges Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Cu-Ni 90/10 Flanges Specifications
| Grade | Copper Nickel 90-10 / UNS C70600 Werkstoff Nr. 2.0872 |
| Standard | ASTM B61, B62, B151, B152 ASME SB61, SB62, SB151, SB152 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 36" |
| Class / Pressure Rating | 150 Class, 300 Class, 90-10 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
Cu-Ni 90/10 Flanges Chemical Composition
| Grade | Cu | Mn | Pb | Ni | Fe | Zn |
| Cupro Nickel 90/10 | 88.6 min | 1.0 max | 0.05 max | 9-11 max | 1.8 max | 1 max |
Cu-Ni 90/10 Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 50000 psi | 20000 psi | 30 % |
Other Types of Cu-Ni 90/10 Flanges Flanges
- Cu-Ni 90/10 Tongue & Groove Flanges Supplier in UAE
- Copper Nickel 90/10 Spectacle blind flanges Manufacturer in India
- Cu-Ni 90/10 Long Weld Neck Flanges
- Cupro Nickel 90/10 Flat Face Flanges
- UNS C70600 High Hub Blind Flanges
- UNS C70600 Lap Joint Flanges
- DIN 2.0872 Reducing Flanges Distributors
- DIN 2.0872 Blind Flanges
- Cupro Nickel 90/10 Slip On Flanges
- Cu-Ni 90/10 Threaded Flanges
- Copper Nickel 90/10 Orifice Flanges Exporter in Russia
- Cu-Ni 90/10 400# Forged Flanges
- Cuppro Nickel 90/10 F91 600# Plate Flanges Supplier in Poland
- UNS C70600 900# Spacer Ring Flanges
- DIN 2.0872 PN6 Nipo Flange in Qatar
- DIN 2.0872 PN10 Nipolet Flanges
- Cupro Nickel 90/10 Pipe Flanges
- UNS C70600 SORF Flanges
- UNS C70600 WNRF Flanges
- Copper Nickel 90/10 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Cupro Nickel 90/10 Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Cupro Nickel 90/10 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo