Stainless Steel 316 Pipes & Tubes
Stainless Steel 316 ERW Seamless Pipe & Tubes, SS 316 Welded Pipe & Tubes, TP316 SS Welded Pipe & Tubes, ASTM A312 TP 316 Tubes, Stainless Steel 316 Pipe & Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading distributor and supplier of Stainless Steel 316 Pipes and Tubes, which endure corrosive environments. Stainless Steel 316 Seamless Pipes is molybdenum-bearing austenitic stainless steels, which is often are added to steel to increase desired properties. The molybdenum gives Stainless Steel 316 Welded Tubes better overall corrosion resistant properties. Stainless Steel 316 EFW Pipes stains less easily than other iron-based metals. These Stainless Steel 316 ERW Tubes are most notable for their corrosion resistance, which increases with increasing chromium content. Stainless Steel 316 Round Pipes is suitable for welding because it has carbon content to avoid carbide precipitation in welding applications.
Stainless Steel 316 Square Tubes has the addition of molybdenum and slightly higher nickel content. Stainless Steel 316 Rectangular Pipes is ideally suited for applications requiring corrosion resistance. Stainless Steel 316 Electropolish Pipes contains molybdenum, which increases their resistance to many chemical corrodents and marine environments. Stainless Steel 316 Hexagonal Tubes offers localized corrosive attack by chlorides and to general corrosion by reducing acids, such as sulfuric acid. Stainless Steel 316 Bush HexPipes has particularly higher resistance to pitting and crevice corrosion in chloride environments. Stainless Steel UNS S31600 Tubes is more resistant to general corrosion and pitting than conventional nickel chromium stainless steels. Stainless Steel WNR 1.4401 Pipes has very high immunity from sensitization (grain boundary carbide precipitation).
UNS S31600, S31609 EFW Pipes & Tubes, SS 316 Seamless Tubes, 316 SS Hallow Pipes & Tubes, SS 316 Hexagonal Pipes, TP 316 Stainless Steel Seamless Pipes & Tubes, TP 316 SS Pipes & Tubes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 316 Pipe Stock Size Range and Specifications
| Grade | SS 316 / TP 316 Stainless Steel Pipes / Stainless Steel 316L / TP 316L Stainless Steel Pipes |
| Size | 1/2" NB - 24" NB |
| Standard | ASTM A/ ASME / SA213 / A249 / A269 / A312 / A358 CL. I to V |
| Form | Round Pipes, Square Pipes, Rectangular Pipe, “U” Shape, Oval Pipes, Hydraulic Pipes |
| Schedule | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW /LSAW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 316 | SS 316L |
| UNS | S31600 | S31603 |
| WERKSTOFF NR. | 1.4401 / 1.4436 | 1.4404 / 1.4435 |
| AFNOR | Z7CND17‐11‐02 | Z3CND17‐11‐02 / Z3CND18‐14‐03 |
| JIS | SUS 316 | SUS 316L |
| GOST | - | 03Ch17N14M3 / 03Ch17N14M2 |
| BS | 316S31 / 316S33 | 316S11 / 316S13 |
| EN | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
316 Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316 – 316L | min. | – | – | – | – | – | 16.0 | 2.0 | 10.0 | – |
| max. | 0.08 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.0 | 14.0 | 0.10 | |
Stainless Steel 316 Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 316 – 316L | 515 | 205 | 40 | 95 | 217 |
Other Types of Stainless Steel 316 Pipes & Stainless Steel Tubes
- SS 316 Seamless Pipes Supplier in UAE
- Stainless Steel 316 Pipes Manufacturer in India
- SS 316 Welded Pipes
- ASTM A312 TP 316 Fabricated Pipes
- Stainless Steel 316 Tubes
- SS 316 Round Tubes
- Stainless Steel 316 Square Pipe
- 316 Electropolish ERW Pipes
- UNS S31600 Hexagonal Pipe
- 316 Stainless Stel Hallow Pipe
- UNS S31600 Welded Tubes Exporter in Russia
- Steel 316 Bush Hex Pipe
- Stainless Steel 316 Round Pipe Supplier in Poland
- SS 316 ERW Pipes
- Stainless Steel 316 EFW Pipes in Qatar
- DIN 1.4401 / 1.4436 Steel Pipes
- Werkstoff Nr. 1.4401 / 1.4436 Steel Tubes
- X5CrNiMo17-12-2 / X3CrNiMo17-13-3 Pipes
- SUS 316 Pipes
- SUS 316 Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 316 Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 316 Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo