Incoloy 800/800H/800HT Pipe & Tubes
Incoloy 800 Pipes & Tubes, ASME SB407 Incoloy 800H Pipe & Tubes, 800 Incoloy Seamless Pipes & Tubes, 800H Incoloy Pipes & Tubes, Incoloy Alloy 800HT Welded Pipes & Tubes, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of leading distributors and suppliers of Inconel Alloy 800 / 800H / 800HT Pipes and Tubes, which is a combination of nickel and chromium alloy. Inconel 800 Seamless Pipes is used for the same creep resistant applications.Inconel 800H Welded Tubes has excellent resistance to suffixation, oxidationand carburization. Inconel 800HT EFW Pipes has greater creep and stress rupture properties. Inconel 800 Round Tubes has significantly higher creep rupture strength, resultant from the close control of the aluminum, carbon, and titanium contents. Inconel 800H Square Pipes resists oxidation, carburization and other high temperature corrosion. Applications of Inconel 800HT Rectangular Tubes have extended from petrochemical processing reformer tubing, to bellows and flare tips in refinery service.
Inconel 800 Electropolish Pipes is an austenitic heat resistant alloy designed for high temperature structural applications.Inconel 800H Hexagonal Tubes has good strength and excellent resistance to oxidation and carburization in high-temperature exposure. Inconel 800HT Hallow Pipes maintains the ultimate chemical properties for high-temperature strength and resistance to oxidation. Inconel 800 Bush Hex Tubes is an iron-nickel-chromium alloy with moderate strength and good resistance to oxidation and carburization at elevated temperatures. Inconel UNS N08811 Pipes is especially useful for high-temperature equipment in the petrochemical industry. Inconel UNS N08800 Tubes has good corrosion resistance in a variety of corrosive environments. Inconel UNS N08810 Pipes doesn't form the embrittling sigma phase after long time exposure at 1200 Degrees F (649 Degrees C).
Incoloy WERKSTOFF NR. 1.4876 Pipe & Tubes, Alloy 800H ERW Pipes, Incoloy UNS N08800 / N08810 / N08811 Welded Pipe & Tubes, ASTM B407 Incoloy 800HT Hollow Pipe, ASME SB407 Seamless Incoloy 800HT Pipes Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 800/800H/800HT Pipe & Tubes Specifications
| Grade | Incoloy 800 / 800H / 800HT |
| Standard | ASTM B407, ASTM B514, ASTM B515, ASTM B775, ASTM B751, ASTM B829 / DIN 17459, BS3 3074NA15, ISO 6207, VdTüV 412 & 434 |
| Incoloy 800/800H/800HT Seamless Pipes | 1/4" NB To 6" NB |
| Incoloy 800/800H/800HT Welded / ERW Pipes | 1" NB To 16" NB |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Incoloy 800 | Incoloy 800H | Incoloy 800HT |
| UNS | N08800 | N08810 | N08811 |
| EN | X10NiCrAlTi32-20 | X5NiCrAlTi31-20 | X8NiCrAlTi32-21 |
| AFNOR | Z8NC32-21 | Z8NC33-21 | - |
| JIS | NCF 800 | NCF 800H | NCF 800HT |
| BS | NA 15 | NA 15(H) | NA 15(HT) |
| WERKSTOFF NR. | 1.4876 | 1.4958 / 1.4876 | 1.4859 / 1.4876 |
| GOST | ЭИ670 | ЭИ670 | ЭИ670 |
| OR | XH32T | XH32T | XH32T |
Incoloy 800/800H/800HT Pipe & Tubes Chemical Composition
| Grade | C | Mn | Si | Fe | S | Cr | Al-Ti | Ni | |
| 800 | min. | – | – | – | 39.5 | – | 19.0 | 0.15 | 30.0 |
| max. | 0.1 | 1.5 | 1.0 | – | 0.015 | 23.0 | 0.60 | 35.0 | |
| 800H | min. | 0.05 | – | – | 39.5 | – | 19.0 | 0.15 | 30.0 |
| max. | 0.1 | 1.5 | 1.0 | – | 0.015 | 23.0 | 0.60 | 35.0 | |
| 800HT | min. | 0.06 | – | – | 39.5 | – | 19.0 | 0.85/0.25 | 30.0 |
| max. | 0.1 | 1.5 | 1.0 | – | 0.015 | 23.0 | 1.20/0.60 | 35.0 | |
Incoloy 800/800H/800HT Pipe & Tubes Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 800-H-HT | Psi – 75,000 , MPa – 520 | Psi – 30,000 , MPa –205 | 30 | – | – |
Other Types of Incoloy 800/800H/800HT Pipe
- Incoloy 800 ERW Tubes Supplier in UAE
- ASTM SB775 Incoloy Tubing Manufacturer in India
- SB829 Incoloy Welded Tubes
- UNS N08810 Seamless Tubing
- ASTM SB775 Incoloy 800HT ERW Pipes
- ASTM SB167 Welded Tubing
- Incoloy 800HT Hydraulic Tubes Distributors
- ASTM SB829 Incoloy Seamless Pipes
- DIN 1.4958 / 1.4876 Round Tubing
- Incoloy 800H Welded Tubes
- Alloy 800 Bush Hex pipe Exporter in Russia
- Alloy N08811 Rectangular Pipe
- Alloy N08800 Seamless Pipes Supplier in Poland
- Incoloy 800 Fabricated Pipes
- UNS N08810 Hexagonal Pipe in Qatar
- 800 Alloy Seamless Pipes
- 800HT Incoloy ERW Pipes
- Incoloy 800 EFW Pipes
- Incoloy N08810 Rectangular Pipe
- Alloy 800HT Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 800/800H/800HT Pipe & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 800/800H/800HT Pipe & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo