Copper Nickel 70/30 Socket Weld Forged Fittings
Copper Nickel 70/30 Socket Weld 90 Deg. Elbow, Cu-Ni 70/30 Socket Weld Tee, UNS C71500 Socket Weld Cross, DIN NR. 2.0882 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a leading Manufacturer, Supplier of Copper Nickel 70 / 30 Socket Weld Forged Fittings, which are available at best possible rates. Being a well-established organization, we are offering a huge range of Cupro Nickel 70 / 30 Socket Weld Elbow Forged Fittings, which is manufactured under the guidance of experts by using superior quality copper. Since Cu-Ni 70 / 30 Socket Weld Tee Forged Fittings is much softer than steel, it bends and flares easier, and the same property allows it to form a better seal with hydraulic components. Copper Nickel 70 / 30 Socket Weld Cap Forged Fittings have been used in auto components, tools for marine exploration and in power plants. Cupro Nickel 70 / 30 Socket Weld Cross Forged Fittings offers tighter controls on impurities and mechanical properties together with a mandatory impact value.
Cu-Ni 70 / 30 Socket Weld Coupling Forged Fittings exhibits outstanding resistance to general and impingent attack by clean sea water. Copper Nickel 70 / 30 Socket Weld Union Forged Fittings has moderate machinability and high impact resistance. Copper Nickel 70 / 30 Socket Weld Plug Forged Fittings is used in desalination plants, ship building, heat exchanger systems and evaporator vessels. Cupro Nickel 70 / 30 Socket Weld Lateral Tee Forged Fittings have good fabricability and high inherent resistance to biofouling.The main and wrought Cu-Ni C71500 Socket Weld Forged Fittings selected for sea water service comprise 30 percent of nickel.
Copper Nickel 70/30 Socket Weld Cap, Cu-Ni 70/30 Socket Weld Bend, Cupro Nickel 70/30 Socket Weld Cross, UNS C71500 Socket Weld Bushing, Cu-Ni 70/30 Socket Weld Coupling, Cupro Nickel 70/30 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Copper Nickel 70/30 Socket Weld Forged Fittings Specifications
| Grade | Copper Nickel 70-30 | UNS C71500 |
| Standard | ASTM B122, ASTM B171, ASTM B466, ASTM B467 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 70-300 LBS, 3000 LBS, 70-300 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Cu-Ni 70-30 |
| UNS | C71500 |
| WERKSTOFF NR. | 2.0882 |
Copper Nickel 70/30 Socket Weld Forged Fittings Chemical Composition
| Grade | Cu | Mn | Pb | Ni | Fe | Zn |
| Cupro Nickel 70/30 | 65 min | 1.0 max | 0.05 max | 29-33 max | 0.4-1.0 max | 1 max |
Copper Nickel 70/30 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 50000 psi | 20000 psi | 30 % |
Other Types of Copper Nickel 70/30 Socket Weld Threaded Forged Fittings
- Copper Nickel 70/30 Socket Weld Forged Elbow Supplier in UAE
- Copper Nickel 70/30 Socket Weld Equal Tee Manufacturer in India
- Cu-Ni 70/30 Socket Weld Cross
- UNS C71500 Socket Weld Union
- UNS C71500 Socket Weld Plug
- Cu-Ni 70/30 Socket Weld Hex Plug
- DIN NR. 2.0882 45 Deg Socket Weld Elbow Distributors
- DIN NR. 2.0882 Socket Weld Bushing
- Cupro Nickel 70/30 Socket Weld Lateral Tee
- Cupro Nickel 70/30 Socket Weld Cross
- Copper Nickel 70/30 Socket Weld Tees
- Cupro Nickel 70/30 45 deg Socket Weld Elbow Supplier in Poland
- Cu-Ni 70/30 Socket Weld 90 deg Elbow
- DIN NR. 2.0882 Socket Weld Cap in Qatar
- DIN NR. 2.0882 Socket Weld Bend Flanges
- Copper Nickel 70/30 Socket Weld Union
- Cupro Nickel 70/30 Socket Weld Bushing
- Cu-Ni 70/30 Socket Weld Lateral Tee
- Cu-Ni 70/30 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Copper Nickel 70/30 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Copper Nickel 70/30 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo