Cu-Ni 70-30 Pipes & Tubes
ASTM B466 Cu-Ni 70/30 Seamless Pipes, Cupro nickel 70/30 ASTM B 151 Welded Tubes, Copper Nickel 70/30 EFW Tubing, Cu-Ni 70/30 Polished Pipes, Cu-Ni 70/30 (C71500) Black Round Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is a distinguished supplier of Copper Nickel 70 / 30 Pipes & Tubes, which are a part of the electronic grade alloy family. Cupro Nickel 70 / 30 Seamless Pipes are a nickel alloy with additions of iron and manganese. Cu-Ni 70 / 30 Welded Tubesoffers excellent corrosion resistance, especially in marine salt water environments. Copper Nickel 70 / 30 EFW Pipes are known for its moderate potency, workability, weldability and formability. Cupro Nickel 70 / 30 ERW Tubesare a copper nickel alloy with excellent resistance to corrosion and erosion. Cu-Ni 70 / 30 Round Pipes are composed of 70 percent of copper and 30 percent of Nickel, with a lower conductivity.
Copper Nickel 70 / 30 Square Tubes provides great resistance to marine water corrosion. Cupro Nickel 70 / 30 Rectangular Pipes have high oxidation resistance and stress corrosion cracking resistance. Cu-Ni 70 / 30 Electropolish Tubes are obtainable in wide-ranging sizes, specifications, lengths, and dimensions so as to suit the precise necessities of our well-regarded customers. Copper Nickel 70 / 30 Hexagonal Pipes is anickel alloy that is almost entirely resistant to stress erosion. Cupro Nickel 70 / 30 Heat Exchanger Tubes are developed for and have been used extensively in seawater applications. Cu-Ni 70 / 30 Hallow Pipes have the heating element of constantan or nickel-chromium alloy within a sheath of copper, cupronickel or stainless steel.
ASME SB 111 Copper Nickel 70/30 Hydraulic Tubes, Cu-Ni 70/30 Capillary Tubes, Copper Nickel 70/30 Square Pipes, DIN 2.0882 Cu-Ni Round Pipes, Copper Nickel 70/30 Rectangular Pipes, Cu-Ni UNS C71500 ERW Tubes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Cu-Ni 70-30 Pipes & Tubes Specifications
| Grade | Copper Nickel 70-30, UNS C71500 |
| Standard | ASTM B111, B151, B466 / ASME SB111, SB151, SB466, MIL-T-16420K, MIL-15005, CN102, C70610, CW352H, DEF STAN 02-879 Annex C, DEF STAN 02-779, NES 779, BS2870, BS2874, ASTM B151, EN 12163, NF A51-115, CuNi10Fe1Mn |
| Size | 1/4" NB To 12" NB |
| Out Diameter Size | 3mm OD to 114.3 mm OD |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Copper Nickel 70-30 |
| UNS | C71500 |
| WERKSTOFF NR. | 2.0882 |
Cu-Ni 70-30 Pipes & Tubes Chemical Composition
| Cu-Ni 70/30 | Cu | Pb | Mn | Fe | Zn | Ni |
| 65.0 min | 0.05 max | 1.0 max | 0.4-1.0 | 1 max | 29 – 33 |
Cu-Ni 70-30 Pipes & Tubes Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 20000 psi | 50000 psi | 30 % |
Other Types of Cu-Ni 70-30 Pipes & Tubes
- Cu-Ni 70-30 Pipes Supplier in UAE
- Cupro Nickel C71500 Seamless Pipes Manufacturer in India
- Cu-Ni 70-30 Welded Pipes
- 70-30 Cu-Ni Hallow Pipe
- Copper Nickel 70-30 Round Pipe
- Cu-Ni 70-30 Fabricated Pipes
- UNS C71500 Hexagonal Pipe Distributors
- Copper Nickel 70-30 Welded Tubing
- DIN 2.0882 Seamless Tubing
- ASTM B151 Hexagonal Pipe
- Copper Nickel 70/30 Seamless Pipes Exporter in Russia
- Copper Nickel 70/30 Seamless Tubing
- UNS C71500 Capillary Tubes Supplier in Poland
- Copper Nickel 70/30 ERW Tubes
- DIN 2.0882 Rectangular Seamless Pipes in Qatar
- Cu-Ni 70/30 Round Pipe
- ASTM B466 Cupro Nickel 70/30 Pipes
- Cu-Ni 70/30 ERW Pipes
- Cu-Ni C71500 Rectangular Pipe
- Cu-Ni 70/30 Pipes
Countries We Export to
Nickel Super Alloys manufactures and exports Cu-Ni 70/30 Pipes & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Cu-Ni 70/30 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo